TECHNET Archives

October 2007

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Mon, 29 Oct 2007 05:32:05 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Creswick, Steven" <[log in to unmask]>
Subject:
From:
"Creswick, Steven" <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (101 lines)
Cantagallo,

Coming from a hybrid background, like Ingemar, when I see DBC, I think
of DBC on alumina substrates. I hope that is what you are speaking of as
well.

I don't have any specific references at my finger tips that I can
forward to you, but will see if I can dig anything up.

My thought is that the higher thermal mass of the DBC substrate will
require more time to preheat thoroughly, and you will have to be more
generous with time above liquidus temperature as well, just to get it
there.

I would think this is a great application for vapor phase soldering.
You might scan the web sites of VP equip manufacturers for tech articles
on DBC soldering, if you had not already done so.

Steve

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Hernefjord Ingemar
Sent: Friday, October 26, 2007 9:26 AM
To: [log in to unmask]
Subject: Re: [TN] Soldering on DBC

Doesn't that depend on what you use DBC for? See below:

http://www.stellarind.com/articles/vapor_deposited_eutectic_solders.pdf

As far as I remember (we've used DBC long ago), DBC is like any PWB
process, except that it's much tougher. With other words, you can solder
even with AuSn, and same way as soldering (brazing)thickfilm on ceramic.


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of
[log in to unmask]
Sent: den 19 oktober 2007 07:24
To: [log in to unmask]
Subject: [TN] Soldering on DBC


Hello Technetters,
I have to look for use of DBC (Direct Bond Copper) substrates for high
reliability applications.
Could anyone give me references of technical articles, books or website
about the soldering (iron and vapor phase) of SMD's and wire connections
with SnPb on DBC ?
What are the main issues we have to survey ?

Thanks in advance,

Best regards,

CANTAGALLO Luigi


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

THE INFORMATION CONTAINED IN THIS E-MAIL MESSAGE AND ANY ATTACHMENTS SENT FROM GENTEX CORPORATION IS GENTEX CONFIDENTIAL INFORMATION INTENDED ONLY FOR THE PERSONAL USE OF THE INDIVIDUAL OR ENTITY NAMED ABOVE. If you are not the intended recipient, you are hereby notified that any review, distribution, or copying of this communication is strictly prohibited.  If you have received this communication in error, please immediately notify the sender by return e-mail, and delete this e-mail message and any attachments from your computer.  




---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2