Phil -
IPC-2221 Table 6-1 covers electrical spacing column B1 applies to bare
boards internal traces. The calculated spacing for 600V would be 0.5mm
[0.020"].
Jeffrey McGlaughlin, CID
Engineering Designer
Battelle
505 King Avenue
Columbus Ohio 43201-2693
(614)424-7582 Phone
(614)458-7582 Fax
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Phil Nutting
Sent: Monday, October 15, 2007 10:29 AM
To: [log in to unmask]
Subject: [TN] inner layer spacing for voltage
Good morning,
One of our engineers posed this question;
" I have an inner ground plane in an area with high voltage (to 600 V).
My question is this: What is the recommended spacing between the
plated-though hole with this voltage and the internal ground plane
relief outline? I will go with 10 V/mil as a default, but I am hoping
the safe limit might be a bit higher than this."
Can you point me to an IPC spec for this? I was thinking it might be in
2222.
Thanks in advance.
Phil
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|