I'm also for the test coupon and always recommended at least
half-a-dozen (preferably more) holes of each diameter, with separate
daisy-chaining for each diameter. A single hole test is statistically
invalid, no matter which test is done. I measured the resistance of each
chain and occasionally did a burn-out test by applying a small voltage
and ramping up the current until one hole burnt out, in a fume cupboard.
This is guaranteed to weed out weak holes, due to poor drilling; even
almost invisible faults by other methods would have fusing currents
dropping by several amps. The coupons can also be used for X-sectioning,
of course.
Brian
Hfjord wrote:
> Gosh! Where did I get that from? Has nothing to do with Uranium. I mean
> My two rems.
>
> -----Ursprungligt meddelande-----
> Från: Hfjord [mailto:[log in to unmask]]
> Skickat: den 13 oktober 2007 22:52
> Till: 'TechNet E-Mail Forum'; [log in to unmask]
> Ämne: SV: [TN] URGENT HELP NEEDED:- non-destructive method for via hole
> plating thickness
>
> Don't know if Feinfocus X-ray has enough resolution, but may be worth
> trying. A Feinfocus fitted with a Hamatsu image processor may fix it. There
> is a contrast difference between Copper and Tin/Lead.
> My two Bequerels
> /Inge
>
> -----Ursprungligt meddelande-----
> Från: TechNet [mailto:[log in to unmask]] För [log in to unmask]
> Skickat: den 13 oktober 2007 18:27
> Till: [log in to unmask]
> Ämne: [TN] URGENT HELP NEEDED:- non-destructive method for via hole plating
> thickness
>
> Hi to all,
>
> Looking for service or friendly (aren't we all) PWB manu. who has the
> capability to measure COPPER plating thickness in via holes in FINISHED
> BRD. i.e.
> with HASL in via holes. NON-DESTRUCTIVE TESTING
>
> Description of brd:-
>
> 20 layers
> ~150 mils thick
> Via holes are 20-22 mils finished.
>
> Required plating is 0.0015 min.
>
> A few I have learnt about are CMI (probe inside the hole) & UPA (resistance
>
> measurement)
>
> Rush
> 818-415-0030
>
>
>
> ************************************** See what's new at http://www.aol.com
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
>
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|