TECHNET Archives

October 2007

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Sat, 13 Oct 2007 23:03:31 +0200
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Hfjord <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
From:
Parts/Attachments:
text/plain (73 lines)
Gosh! Where did I get that from? Has nothing to do with Uranium. I mean 
My two rems.

-----Ursprungligt meddelande-----
Från: Hfjord [mailto:[log in to unmask]] 
Skickat: den 13 oktober 2007 22:52
Till: 'TechNet E-Mail Forum'; [log in to unmask]
Ämne: SV: [TN] URGENT HELP NEEDED:- non-destructive method for via hole
plating thickness

Don't know if Feinfocus X-ray has enough resolution, but may be worth
trying. A Feinfocus fitted with a Hamatsu image processor may fix it. There
is a contrast difference between Copper and Tin/Lead.
My two Bequerels
/Inge

-----Ursprungligt meddelande-----
Från: TechNet [mailto:[log in to unmask]] För [log in to unmask]
Skickat: den 13 oktober 2007 18:27
Till: [log in to unmask]
Ämne: [TN] URGENT HELP NEEDED:- non-destructive method for via hole plating
thickness

Hi to all,
 
Looking for service or friendly (aren't we all) PWB manu. who has the  
capability to measure COPPER plating thickness in via holes in FINISHED
BRD.  i.e. 
with HASL in via holes.  NON-DESTRUCTIVE TESTING
 
Description of brd:-
 
20 layers
~150 mils thick
Via holes are 20-22 mils finished.
 
Required plating is 0.0015 min.
 
A few I have learnt about are CMI (probe inside the hole) & UPA  (resistance

measurement)
 
Rush
818-415-0030



************************************** See what's new at http://www.aol.com

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2