Once upon a time I used a nasty chemical to confirm voids within a plastic delay package. The experiment was very successful and supported our cause. The sample was submerged in this chemical and placed under vacuum and then x-ray. The chemical is very heavy and more dense than lead. Therefore, the plastic package would reveal signs of this chemical entry and cavity fill.
Victor,
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Thursday, October 11, 2007 7:38 AM
To: [log in to unmask]
Subject: Re: [TN] Cracks in the body of glass diodes (JANTX1N4148UR1)
Good Morning Juan!
I have your pictures posted. They are here:
http://stevezeva.homestead.com/files/JTX1N4148_UR1_003.jpg
http://stevezeva.homestead.com/files/JANTX1N4148_UR1_004.jpg
http://stevezeva.homestead.com/files/JANTX1N4148_UR1_001.jpg
I'm with Inge on this one. These cracks are in the body, not good. There is something I have noticed in two of the pictures, UR1_004 and UR_001, is that the glass seems discolored right next to the termination, which to me indicates that they may have been thermally shocked.
Do you know where these diodes were purchased from? Brokers maybe? Maybe salvaged off some boards? Poorly pre-tinned to restore solderability?
I wouldn't use them...
Steve Gregory
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Juan T. Marugán
Sent: Thursday, October 11, 2007 5:25 AM
To: [log in to unmask]
Subject: [TN] Cracks in the body of glass diodes (JANTX1N4148UR1)
Good Morning,
In a certain number of SMD diodes we have detected what we consider as a crack in the glass body of the diode. This condition was already present in the diodes packaged in a reel, that is, before mounting in the PWAs.
What we cannot determine yet is if this condition could be acceptable. Could you help us through your valuable opinions?
PD: I have sent 3 photographs to Steve Gregory.
Thank you in advance.
Juan T. Marugán López
Indra Sistemas SA
Supply Chain Management (SCM)
Production Quality
C/ Joaquín Rodrigo 11
28300 Aranjuez - Madrid (SPAIN)
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|