TECHNET Archives

October 2007

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Juan T. Marugán <[log in to unmask]>
Date:
Thu, 11 Oct 2007 14:02:28 +0200
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Hernefjord Ingemar <[log in to unmask]>
Subject:
From:
Hernefjord Ingemar <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (45 lines)
Juan,
why should you accept cracked diodes at all? If the glass is in that condition, something is VERY wrong! I've seen all models of glass diodes since the very first ones, and only seen a few cases with glass cracks. We use to have too defintions: glass cracks and glass chipouts. If the 'cracks' are just micro chipouts at the lead entrance in the glass, you may accept the diodes, because such cracks do not hazard the hermetic seal of the chip. However, if the crack is in the body around the chip, you can't use the diodes, because the hermeticity is lost, and you understand the consequencies, don't you? There are standards about this, but I don't have it at the moment.
/Regards
Inge

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Juan T. Marugán
Sent: den 11 oktober 2007 12:25
To: [log in to unmask]
Subject: [TN] Cracks in the body of glass diodes (JANTX1N4148UR1)


Good Morning,

In a certain number of SMD diodes we have detected what we consider as a crack in the glass body of the diode. This condition was already present in the diodes packaged in a reel, that is, before mounting in the PWAs.

What we cannot determine yet is if this condition could be acceptable. Could you help us through your valuable opinions?

PD: I have sent 3 photographs to Steve Gregory.

Thank you in advance. 

Juan T. Marugán López
Indra Sistemas SA
Supply Chain Management (SCM)
Production Quality
 
C/ Joaquín Rodrigo 11
28300 Aranjuez - Madrid (SPAIN)
 

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2