Ability to repair, spare parts conformance, outgassing, weight,
wettability to metals, wettability to platings, wettability to plastics,
ageing aspects, temperature change, max/min operating temperature,
viscosity important for complex parts, recycling aspects, cleanliness
before coating/potting, curing method (air/UV/heat etc), hardness
(shore), dielectric properties (RF circuits), humidity absorption, salt
spray withstanding, UV resistibility (sun), contamination proof
(corrosive ambient), level of air inclusions, volumetric
expansion/contraction, fire aspects....example on things to think of.
/Inge
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Tempea, Ioan
Sent: den 10 september 2007 21:08
To: [log in to unmask]
Subject: [TN] Conformal coating/potting DfA
Dear Technos,
what would be the Design for Assembly concerns related to products that
will be conformally coated or potted?
Thanks,
Ioan
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|