Lenny Carter <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Wed, 5 Sep 2007 13:03:27 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (56 lines)
not in my opinion.  this is fine.  I think the verbiage IPC uses is that the 
lead must be discernable in the solder joint, and .040" will be plenty 
discernable.  If you are worried about mechanical reliability of the joint I 
bet you could subject this joint to any stress you would be able to subject 
a .040" longer lead protrusion to.
my $.02.
Lenny Carter
Design Engineer
ERG, Inc.
www.ergpower.com


----- Original Message ----- 
From: "Phil Nutting" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Wednesday, September 05, 2007 11:17 AM
Subject: [TN] Connector pin protrusion


Good Afternoon,

In reviewing PTH connectors it looks like the standard pin length (for
the through board connection) is double the board thickness.  For an
0.062 board the pins are 0.120" long and for a 0.090 board the pins are
0.180" long.  We have some connectors that have 0.130" long pins that we
want to use in an 0.090" thick board.  I maintain this shorter pin will
be problematic to solder reliably.

Am I on the right track?

Phil

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2