I'm confused by this, probably because I'm not knowledgeable on plasma
cleaning. But so far as I understand this area, the principal uses of plasma
are
- ash off surface contamination to get a clean surface,
Or
- it can be used to impregnate or burn surfaces to make them 'active' (eg
to make PTFE bondable with adhesive)
It depends (!) on the type of plasma and energies used.
This seems to be a confusion of these two functions. Oxidising epoxy would
make a carbon rich layer, oxidizing silver would make silver oxide, both AgO
and C are conductive so we have weakly conductive substrate.
This is a powered device so we have some volts,. The only missing item for
Ag migration is a little damp.
Altogether: not a recipe for high reliability. Or did I miss something?
Regards
Mike
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Hernefjord Ingemar
Sent: Friday, August 31, 2007 9:53 AM
To: [log in to unmask]
Subject: [TN] Plasma "oxidation"
Yup. Strange title. I've been asked about a strange process, which one
was introduced without my knowledge, and I'm going to throw it out. But
I thought of consulting TN before. This is the case:
LTCC substrates are silver epoxy dispensed for chip mounting. In order
to avoid risk for silver migration, a guy invented plasma "oxidation",
i.e. he use a plasma cleaner, runs Argon with 6% Oxygen for a couple of
minutes on mounted substrates. The silver epoxy dots become blackish
because of oxidation, and oxidized epoxy is meant to minimize risk for
silver migration. The oxide is of course just nanometer thick. The guy
worked at a wafer manufacturing plant and had experience of cleaning
procedures.
I mean that this process is nonsense. If humidity gets in and condense
on the substrate, and if the electric field is high enough, and if there
are salts or contaminations, there is still enough silver to start
migration. Oxidation of the silver dot's surface is meaningless. Anyone
heard of such a strange process? Plasma operation on mounted LTCC
substrates is foreign to me, I want it out.
TrikeMan?
Inge
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
***This email, its content and any files transmitted with it are intended solely for the addressee(s) and may be legally privileged and/or confidential. If you are not the intended recipient please delete and contact the sender by return and delete the material from any computer. Any review, retransmission, dissemination or other use of, or taking of any action in reliance upon, this information by persons or entities other than the intended recipient is prohibited.
Messages sent via this medium may be subject to delays, non-delivery and unauthorized alteration. This email has been prepared using information believed by the author to be reliable and accurate, but Indium Corporation makes no warranty as to accuracy or completeness. In particular, Indium Corporation does not accept responsibility for changes made to this email after it was sent. Any opinions or recommendations expressed herein are solely those of the author. They may be subject to change without notice.***
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|