TECHNET Archives

September 2007

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Fri, 28 Sep 2007 09:05:54 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Kevin Glidden <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="US-ASCII"
From:
Kevin Glidden <[log in to unmask]>
Parts/Attachments:
text/plain (29 lines)
We recently received a shipment of PCBs where the exposed outer layer
laminate has staining that looks like copper. I have a photo -
<http://tinyurl.com/yp9za2> http://tinyurl.com/yp9za2
My question is what would cause this?  I've never seen it before, but I am
thinking something in the Copper plating process.  The vendor is telling us
it is staining but it is an asthetic issue only. What would cause it?  Is it
an asthetic issue only?  It seems to me if the staining was caused by some
plating chemistry, then it would effect the laminate properties,
particularly the insulation resistance.
 
Thanks!
 
Kevin Glidden
Manufacturing Engineer
Luminescent Systems Inc.
 
 
 

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2