Hi Gil!
That's the way I like my failures! Very dramatic!
We can presume that the observed phenomenon is the result of too much
current going through too little conductor. How did that much current
get there? To answer that question, you must first draw a "fishbone"
diagram which shows how many different ways you could get current in the
offending conductor high enough to cause it to melt. For example, a
partial list:
-failed component on surface of the board
-overcurrent on board I/O
-reduction in cross sectional area for the conductor which melted
(unlikely, but possible)
-mechanical damage to board causing internal short
-CAF or other migration path
-overvoltage resulting in arcing and build-up of carbon deposits
You get the idea. Then you form a consensus on the most likely/quickest
or cheapest to diagnose and weed out those fast. After those are weeded
out, you re-investigate all of the data and come up with
experiments/research to indicate probabilities of the items on the list
you couldn't eliminate yet.
If your real question is whether CAF could do that, yes it can. It
should definitely be on the list. Unfortunately, it sounds like the
"smoking gun" probably got smoked a little too much. But not to worry
since extended bias/humidity testing with the remaining pieces of
circuit board may be able to generate additional conductive paths for
you to analyze.
Wayne Thayer
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Zilber Gil
Sent: Tuesday, September 04, 2007 1:26 PM
To: [log in to unmask]
Subject: [TN] Help needed on motherboard failure analysis
Hi,
Recently one of our motherboard failed. It reaches very high temperature
that melts the copper and explodes shooting (from the side of the board)
the melt copper to over 20 cm. the shooting hole cause delamination of
the board in the area. A lot of black smoke and was also seen. The max
voltage of the board is about 50V. The board worked fine for more then a
year. What could be the failure mechanism? Could it be due to conductive
filament formation (although the PCB should be free of that)?
Thanks
Gil Zilber
Elta Systems
The information contained in this communication is proprietary to
Israel Aerospace Industries Ltd.
and/or third parties, may contain classified or privileged information,
and is intended only for the use of the intended addressee thereof. If
you are not the intended addressee, please be aware that any use,
disclosure, distribution and/or copying of this communication is
strictly prohibited.
If you receive this communication in error, please notify the sender
immediately and delete it from your computer. Thank you.
This message is processed by the PrivaWall Email Security Server.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|