TECHNET Archives

September 2007

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Wed, 12 Sep 2007 14:47:32 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Subject:
From:
Jason Roetz <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (273 lines)
FYI,

Lead shot has been banned from waterfowl hunting nationwide since '91.

Here's the currently approved list of shot types approved for waterfowl
hunting:

bismuth-tin 
 
iron (steel) 

iron-tungsten 
 
iron-tungsten-nickel 
 
tungsten-bronze 

tungsten-iron-copper-nickel 

tungsten-matrix 

tungsten-polymer 
 
tungsten-tin-iron 

tungsten-tin-bismuth 

tungsten-tin-iron-nickel 




-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ian Hanna
Sent: Wednesday, September 12, 2007 1:44 PM
To: [log in to unmask]
Subject: Re: [TN] Military Exemption from Lead-Free?

Hopefully (?) there is a huge difference between the amount of dropped
shot and dropped bullets...

would bismuth-tin in this case be any easier on the gizzards?



-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Bev Christian
Sent: Wednesday, September 12, 2007 2:27 PM
To: [log in to unmask]
Subject: Re: [TN] Military Exemption from Lead-Free?

John,
I am glad they are banning lead for hunting bullets.  As I have noted
here on this or the LeadNet forum, lead shot has been a big problem in
states like Minnesota.  Most of the shot does not end up in birds (then
picked out while they are being prepared to be eaten or while eaten -
ouch), but in shallow marshes where the migrating water fowl eat it
thinking it is grit/small stones that their gizzards can use to grind
their food. Ironically they die - not directly of lead poisoning, but of
starvation, as the lead destroys the functioning of their gizzard.

Bev
RIM

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of John Burke
Sent: Wednesday, September 12, 2007 2:01 PM
To: [log in to unmask]
Subject: Re: [TN] Military Exemption from Lead-Free?

I believe it should be illegal to bomb the World with poorly thought out
lead free legislation........................8-)

By the way California passed a law this week to ban lead in bullets for
hunting .............

 
 
John Burke
 
(408) 515 4992
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ian Hanna
Sent: Wednesday, September 12, 2007 8:36 AM
To: [log in to unmask]
Subject: Re: [TN] Military Exemption from Lead-Free?

Wouldn't it though be illegal to bomb a country with lead-free
legislation in place unless the weapons systems were compliant?

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Genny Gibbard
Sent: Wednesday, September 12, 2007 11:19 AM
To: [log in to unmask]
Subject: Re: [TN] Military Exemption from Lead-Free?

Military is not EXEMPT, it is OUT OF SCOPE.   The directive does not
apply at all to military (other than the indirect massive impact the
directive has had).  The directive has no legislative control over
military electronics.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard D.
Sent: September 12, 2007 8:10 AM
To: [log in to unmask]
Subject: Re: [TN] Military Exemption from Lead-Free?

No specific alloy is "forbidden" in military electronics. 
In general, solders and fluxes are categorized per and must comply with
J-STD-004, J-STD-005, and J-STD-006.
Specific solder alloy types are called out on assembly prints and BOMs
per MIL-STDs and Weapon Specs.
Military, traffic control, industrial safety, some medical, and many
other products are exempt per RoHS and IEEE exemptions.
  

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Dave Dixon
Sent: Wednesday, September 12, 2007 8:33 AM
To: [log in to unmask]
Subject: Re: [TN] Military Exemption from Lead-Free?

Check out
Air Force's Airworthiness Advisory AA-05-01 It isn't very forceful in
the wording, but is the closest thing I could find so far to support my
cause.  If anyone knows of any documentation forbidding lead free in
military products, I would sure appreciate a heads-up.
Thanks,
Dave

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of ekalgren
Sent: Tuesday, September 11, 2007 3:06 PM
To: [log in to unmask]
Subject: Military Exemption from Lead-Free?

I believe that I remember someone mentioning a military end-use
exemption from lead free requirements.  Am I remembering correctly or is
this just wishful thinking?  If it is true, can anyone point me in the
direction to get it in writing?

 

Thanks!

 

Eric Kalgren

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential
information, privileged material (including material protected by the
solicitor-client or other applicable privileges), or constitute
non-public information. Any use of this information by anyone other than
the intended recipient is prohibited. If you have received this
transmission in error, please immediately reply to the sender and delete
this information from your system. Use, dissemination, distribution, or
reproduction of this transmission by unintended recipients is not
authorized and may be unlawful.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2