Werner,
The "It Depends" clause catches every thing. There must be some
acceptable guideline set forth by IPC. What happened to the 20% of
core thickness statement as per IPC-A-600E.
Victor,
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Werner Engelmaier
Sent: Thursday, August 09, 2007 10:08 AM
To: [log in to unmask]
Subject: Re: [TN] IPC-A-600F, Sec 4.2.6, Core Bond to
Plated-Through-Hole Wall
Hi Victor,
Criteria cannot be set, because "It Depends" (according to Doug Pauls)
on too
many variables. These variables are in no particular order: barrel Cu
thickness, CTE(post-Tg) of laminate and B-stage layers, resin content
(B-stage) Tg,
T reached above Tg, drilled hole diameter, surface land diameter,
surface
land Cu thickness, PCB thickness, non-functional lands, dielectric
spacing.
An actual assessment can only be done with FEA provided REAL properties
are
being used (I have yet to see this).
Werner
**************************************
Get a sneak peek of the all-new AOL at
http://discover.aol.com/memed/aolcom30tour
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|