Silver oxides are highly conductive - but I do not believe the sulphides
are.....................8-)
John
John Burke
(408) 515 4992
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Gerald Gagnon
Sent: Wednesday, August 08, 2007 11:57 AM
To: [log in to unmask]
Subject: [TN] Dry Cicruit Low Level Contact Resistance of Immersion Silver
Hello All,
We are looking at a surface presure contact application between an EMI/RFI
braid against an immersion silver surface finish that has undergone 2 SMT
and 1 wave process.
I know the immersion silver oxidizes (tarnishes) but everything I read
indicates that the oxide is also highly conductive.
Still, I was wondering if the long time users of immersion silver have come
across LLCR data for immersion silver as well as LLCR of the oxide.
TIA
Gerry
_________________________________________________________________
Learn.Laugh.Share. Reallivemoms is right place!
http://www.reallivemoms.com?ocid=TXT_TAGHM&loc=us
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------