After having these crystals analyzed by an outside lab it has been
confirmed that they are definitely Bioact crystals. I had already sent
the boards out for evaluation prior to receiving Joe's email or I
could've saved the $1000 bucks. Thanks anyway for the reply Joe.
Now I just have to determine if they pose any reliability issues for
other boards that may the same condition that have been shipped
already...
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Kane, Joseph E (US
SSA)
Sent: Monday, August 06, 2007 12:43 PM
To: [log in to unmask]
Subject: Re: [TN] Strange crystal growth
Freaky looking, aren't they?
I saw this once years ago. We had cleaned a batch of boards with Bioact
EC-7R in a dishwasher-type system, and the boards then sat undisturbed
over a weekend, unrinsed, because someone forgot about them.
I think these are Bioact crystals, if you can believe that. One more
trip through the Bioact wash will make them disappear.
-Joe
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Brian Ellis
Sent: Wednesday, August 01, 2007 10:45 AM
To: [log in to unmask]
Subject: Re: [TN] Strange crystal growth
Indeed strange. Very few crystals have this acicular form, except metal
whiskers. My first reaction is have them analysed!
Brian
Davis, Larry wrote:
> We have a strange problem here and I was hoping someone could provide
an
> explanation. I had Steve post a couple pictures to his site for
> viewing, thanks Steve!
>
> We are seeing this crystalline growth all over a single assembly that
> was built back in Feb 07 and shipped to one of our customers who kept
it
> stocked in the original esd bag. They noticed it once it was required
> for use and returned it to us. The only thing in our process that I
> think could possibly be the root cause is that our board cleaner
solvent
> (Bioact EC-7R) was getting very flux loaded about that time but we
> haven't seen this on any other assemblies that have been built since
> then. We are using no-clean fluxes and only clean boards that have
high
> impedance circuitry. I find it very strange that the growth occurs on
> the plastic parts as well as the leads of components. Any ideas?
>
> http://stevezeva.homestead.com/files/crystal_growth.jpg
>
> http://stevezeva.homestead.com/files/crystal_growth_closeup.jpg
>
>
> Thanks in advance for your feedback!
>
> Larry Davis
> Hach Co.
>
>
> This message (including any attachments) contains confidential and/or
> proprietary information intended only for the addressee.
> Any unauthorized disclosure, copying, distribution or reliance on the
> contents of this information is strictly prohibited and may constitute
> a violation of law. If you are not the intended recipient, please
> notify the sender immediately by responding to this e-mail, and delete
> the message from your system. If you have any questions about this
> e-mail please notify the sender immediately.
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
> unsubscribe, send a message to [log in to unmask] with following text
in
> the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt
> or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
http://listserv.ipc.org/archives
> Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
> -----------------------------------------------------
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
This message (including any attachments) contains confidential
and/or proprietary information intended only for the addressee.
Any unauthorized disclosure, copying, distribution or reliance on
the contents of this information is strictly prohibited and may
constitute a violation of law. If you are not the intended
recipient, please notify the sender immediately by responding to
this e-mail, and delete the message from your system. If you
have any questions about this e-mail please notify the sender
immediately.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|