Ahhh, I love the sound of a Deweyism early in the Morning. All the
questions on adhesives and now this bonding too; what a cohesive group.
A friend of mine's wife didn't want to dignify what we did when we got
together with the term Male Bonding, so she called it "weiner welding".
Since she hated my Deweyisms, I would always reply "you always think the
wurst".
Dewey
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Phil Nutting
Sent: Friday, August 17, 2007 6:49 AM
To: [log in to unmask]
Subject: Re: [TN] NTC Seeking design information on PWB conductor
spacing for high voltage (500-1000 VDC) applications
Ahhh, a Deweyism. Very good.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Hernefjord Ingemar
Sent: Friday, August 17, 2007 9:46 AM
To: [log in to unmask]
Subject: Re: [TN] Seeking design information on PWB conductor spacing
for high voltage (500-1000 VDC) applications
with such good marginals, one will phil nuthing when heat is on...
Inge
-----Original Message-----
From: Phil Nutting [mailto:[log in to unmask]]
Sent: den 17 augusti 2007 14:30
To: TechNet E-Mail Forum; Hernefjord Ingemar
Subject: RE: [TN] Seeking design information on PWB conductor spacing
for high voltage (500-1000 VDC) applications
To add to this, we will frequently route a slot between two traces or
pads to increase the creepage clearance when a large physical distance
is not possible.
For numbers we use 10 kV per inch for surface creepage and clearance in
air.
For boards submerged in dielectric oil we use 20 kV for surface creepage
and 50 kV for clearance in oil.
For hipot tests (4 kV) to satisfy medical requirements we use 8 mm
spacing between SELV and ground.
Conformal coating can help, but we typically don't need it.
Phil
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Hernefjord Ingemar
Sent: Friday, August 17, 2007 3:07 AM
To: [log in to unmask]
Subject: Re: [TN] Seeking design information on PWB conductor spacing
for high voltage (500-1000 VDC) applications
We have a rather simple thumb rule for top conductors:
flashover 1,250 VDC/mm for dry air
flashover 2,500 VDC/mm for solder mask
flashover 7,500 VDC/mm for potted board
to avoid creep current you need following distance between top
conductors:
7 mm/kV up to 3,000 meter altitude without protection, clean air
15 mm/kV up to 3,000 meter " " " , dusty air
25 mm/kV up to >3,000 meter " " " , std environment
5 mm/kV up to 3,000 meter " with protection, std environment
2.5 mm/kV up to >3,000 meter " " " "
We make MIL products, UL and other commercial requirements are of course
different.
The cleanliness of the boards is mainly the deciding basis for the
isolation distances.
This information is based on rather old stuff, but I think not much is
changed.
Inge
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Gerald Bogert
Sent: den 17 augusti 2007 00:24
To: [log in to unmask]
Subject: [TN] Seeking design information on PWB conductor spacing for
high voltage (500-1000 VDC) applications
August 16, 2007
IPC-2221 section 6.3 and the associated table provides specific
electrical conductor spacing requirements for voltages up to 500 volts.
However, for voltages > 500 volts, it defaults to a formula in section
6.3.
What is the technical basis for the minimum spacing requirements that
are
listed in the table? How reliable is the formula for voltages > 500
volts.
How valid is the formula if we have 1000 VDC on the PWB?
Since the table does not specifically list minimum electrical spacing
for voltages > 500 volts is the formula just a "SWAG" or based on real
data? If so, what is the formula based on?
Does anyone have design standards for high voltage PWB spacings that
they are willing to share?
We had an OEM that had recent field failures (shorts to internal traces)
of a conformal coated multilayer FR4 PWB (0.062 in) that has both low
(logic
voltage) and high (approx 780 VDC nominal) circuits. The board was
required to be designed to IPC-D-275 requirements, and the table in 275
is basically the same as in IPC-2221.
The PWB is being redesigned and I need to verify the new design meets
reliable and valid minimum conductor spacing requirements. Are there
any design standards other than IPC-2221 that could be used for high
voltage PWB?
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|