Forgot to add this as well:
http://www.smta.org/smtai/tech.cfm
|----------------------------------------------------------------------------------------------------|
| |
| |
| |
| |
| |
| |
| |
| |
| |
| |
| |
| SUB2 |
| Effects of Severe Environments on Exposed Circuitry |
| Chair: Donald Cullen, MacDermid, Inc. |
| Co-Chair: Dave Hillman, Rockwell Collins |
| Wednesday, October 10 |
| 10:00am – 11:30am |
| Osceola 3 |
| |
| Immersion silver has been widely employed as a flat, readily solderable, Pb-free circuit |
| finish, especially where surface conductivity is desired. The surface functionality of |
| immersion silver can be used for areas of exposed metal after final assembly. HASL |
| alternatives are thin and can be attacked by environmental pollutants in aggressive |
| industrial environments. Where the underlying copper is exposed, metal "creep" can result |
| in shorts. Our speakers are intent on characterizing the creep corrosion mechanism, show |
| the severity and occurrence in high volume manufacturing, and demonstrate solutions for |
| corrosion prevention. |
| |
| Silver and Sulfur: Case Studies, Physics and Possible Solutions |
| Craig Hillman, Ph.D.; DfR Solutions |
| The Definition, Induction and Correction of Creep Corrosion on Electronic Assemblies |
| Lenora Toscano and John Swanson, MacDermid, Inc. |
| Creeping Corrosion of Immersion Silver in High Sulfur Environments |
| Randy Schueller, Ph.D.; Dell, Inc. |
| |
| |
| |
|----------------------------------------------------------------------------------------------------|
Cheryl Tulkoff
Senior Reliability Engineer
Phone:(512) 683-8586
Fax: (512) 683-8520
National Instruments
11500 N. Mopac Expressway
Building C
Austin, TX 78759-3504
"Wenger, George
M."
<George.Wenger@an To
drew.com> "TechNet E-Mail Forum"
<[log in to unmask]>, "Cheryl Tulkoff"
08/10/2007 07:30 <[log in to unmask]>
PM cc
Subject
RE: [TN] Silver PCB finish and
reliability (question)
Cheryl,
When you indicate a quick Google search on the topic, what topic are you
referring to? Copper creep is typically a thermal issue with copper
alloys and I'm not sure I've every seen it related to immersion silver
surface finish.
Regards,
George
George M. Wenger
Andrew Corporation Wireless Network Solutions
Senior Principal FMA / Reliability Engineer
40 Technology Drive, Warren, NJ 07059
(908) 546-4531 [Office] (732) 309-8964 [Cell]
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Cheryl Tulkoff
Sent: Friday, August 10, 2007 6:30 PM
To: [log in to unmask]
Subject: Re: [TN] Silver PCB finish and reliability (question)
Carl -
Immersion silver is our finish of choice for most of our PCBs - both
leaded
and lead free. There is one known reliability issue referred to as
"copper
creep." In customer environments with high sulfur along with humidity
and
air flow, you can get catastrophic failures. This usually affects vias
or
other areas where there is no solder over the silver. Both Dell and HP
have
published on the topic and we have confirmed failures due to the problem
as
well. We have been working with the immersion silver finish suppliers on
potential improvements.
Industries like tire manufacture, water treatment, paper processing etc.
are likely candidates for problems.
You can do a quick google search on the topic. If you cannot locate the
papers, you can contact me for more details.
Cheryl Tulkoff
Senior Reliability Engineer
Phone:(512) 683-8586
Fax: (512) 683-8520
National Instruments
11500 N. Mopac Expressway
Building C
Austin, TX 78759-3504
Carl VanWormer
<[log in to unmask]>
Sent by: TechNet
To
<[log in to unmask]> [log in to unmask]
cc
08/10/2007 04:07
Subject
PM [TN] Silver PCB finish and
reliability (question)
Please respond to
TechNet E-Mail
Forum
<[log in to unmask]>
; Please respond
to
Carl VanWormer
<[log in to unmask]>
For non-BGA, surface mount boards, we have always ordered HASL boards.
In
our progress towards ROHS compliance, management has changed the default
specification to ENIG. Our board house has HASL, ENIG, and Silver as
options, with Silver at about the same price as HASL and ENIG with a
significant premium (along with a 2 to 3 days added to the processing
time). When I asked management why we couldn't use Silver, I was told
that
there are significant problems with the Silver processed boards (with no
real explanation).
My question to the Group: Is there any good reason to avoid Silver as a
surface finish on my consumer and industrial boards?
Your scary stories are welcomed . . .
Thanks,
Carl
Carl Van Wormer
Cipher Systems
1800 NW 169th Place, Suite B-100
Beaverton, OR 97006
Phone (503)-617-7447 extension 20
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
------------------------------------------------------------------------------------------------
This message is for the designated recipient only and may
contain privileged, proprietary, or otherwise private information.
If you have received it in error, please notify the sender
immediately and delete the original. Any unauthorized use of
this email is prohibited.
------------------------------------------------------------------------------------------------
[mf2]
|