TECHNET Archives

August 2007

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"David D. Hillman" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Fri, 10 Aug 2007 16:23:15 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (90 lines)
Hi Carl - Rockwell Collins has been utilizing immersion silver as a pwb 
surface finish for over 10 years in a wide variety of avionics use 
environments. All pwb surface finishes have specific conditions and use 
environments that they will not work in but the generalization on the 
applicability of immersion silver provided by your management is 
incorrect.


Dave Hillman
Rockwell Collins
[log in to unmask]




Carl VanWormer <[log in to unmask]> 
Sent by: TechNet <[log in to unmask]>
08/10/2007 04:07 PM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
Carl VanWormer <[log in to unmask]>


To
[log in to unmask]
cc

Subject
[TN] Silver PCB finish and reliability (question)






For non-BGA, surface mount boards, we have always ordered HASL boards.  In 
our progress towards ROHS compliance, management has changed the default 
specification to ENIG.  Our board house has HASL, ENIG, and Silver as 
options, with Silver at about the same price as HASL and ENIG with a 
significant premium (along with a 2 to 3 days added to the processing 
time).  When I asked management why we couldn't use Silver, I was told 
that there are significant problems with the Silver processed boards (with 
no real explanation). 

My question to the Group:  Is there any good reason to avoid Silver as a 
surface finish on my consumer and industrial boards? 

Your scary stories are welcomed . . .

Thanks,
Carl





Carl Van Wormer
Cipher Systems
1800 NW 169th Place, Suite B-100
Beaverton, OR  97006
Phone (503)-617-7447 extension 20 




---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
-----------------------------------------------------


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2