Daughter dropped hers into a pond while looking at frogs. I told her to
immediately remove the battery (prevent electrolytic corrosion!), rinse
it in DI water and leave it in as many bits as possible to dry out. The
following day, it was reassembled and it worked perfectly and continued
that way until she lost it in Cambodia 18 months later.
Brian
Anil Kher wrote:
> my cell fell in puddle of water ( its raining heavy in Goa) the authorised
> repair centre told me the LCD panel is bust.
>
> with all knowledge from u gurus I know it cannot happen as electronics is so
> rugged today. so I open it up, separate the PCBs remove the camera and
> ultrasonic clean the assemblies in pure IPA. Bake at 75 degC for 1 hour and
> its OK.
>
> So thanks to all of u. saved 400$.
>
> Could I have done better?
>
> Anil kher
>
> micro interconnexion pvt.ltd.
> D3-12A, Corlim Industrial Estate,
> Corlim, Ilhas, Goa, India - 403110.
> Tel +91-832-2284209/337. Fax +91-832-2284209
> e-mail option - [log in to unmask]
>
> Leaders in Gold Plated PCBs
>
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|