Technet:
A "proper" defoamer is one which is not soluble in the use solution, but becomes soluble in the rinses...
This type is known as a polyglycol, and it has this characteristic because it is inversely soluble with temperature, the higher the temperature, the less soluble. Did I mention that a defoamer needs to be insoluble to function. Polyglycols are insoluble in warm solution, but in cold rinses, become soluble, thus rinsing easily, thus making the level being used less critical.
Rudy Sedlak
Brian Ellis <[log in to unmask]> wrote: I agree with Rudy, especially about temperature. However, if your first
water is too hot, depending on the flux chemistry, the cleaning quality
may be less good. This is especially so if the flux activator contains
amino acids or their derivatives. The ideal temperature is 55-60°C, no
higher.
You can buy defoamer from flux manufacturers, but add minimal
quantities. This is not a case of a little is good, so a lot must be
better. Alternatively, you can make your own. I quote my book:
"Dissolve 300 g soft white soap in one litre of hot water. When cool,
add one litre of octyl alcohol. Shake before use. Add the minimum dose
to obtain the desired effect, usually about 0.1 cm3/l"
Brian
Rob Strecker wrote:
> All,
>
> Has anyone else had foaming issues in an aqueous wash batch cleaner?
> What are some of the causes of excess foaming? We are applying our wave
> flux via spray; however this flux is also suitable in foaming flux
> applications. We are currently in the process of optimizing our flux
> application in the wave to significantly reduce the flux residue on the
> boards. This includes optimizing the sprayers, preheats and dwell time.
> Initial tests show this is not having a major impact in reducing the
> foaming. We will be testing boards with only SMT flux residue, then
> ones with only wave flux residue. The theory is that by themselves they
> do not foam but when mixed cause foaming. We have recently changed
> Paste suppliers, thus we now have two different manufactures of flux
> mixing in the wash (one from SMT, one from wave). Could this be a cause
> of excessive foaming?
>
>
>
> Thanks,
>
> Rob Strecker
>
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------
Need a vacation? Get great deals to amazing places on Yahoo! Travel.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|