Unless other factors prohibit,
I would just drill an unplated hole
in the "corner" (which happens
before routing), and let the vendor
use their typical .06 radius.
Absolutely no cost adder, free.
Jack
p.s. some vendors are using smaller
router bits now, because they don't
want to spend their energy grinding
out large amounts of fiberglass for
no reason.
On 8/2/07, David Baldwin <[log in to unmask]> wrote:
>
> DC Members:
>
> I am designing a board that has a critical inside corner. Can anyone
> tell me what the typical minimum routing bit that a board shop
> uses? I need a perfect corner so I believe we will need to overshoot
> the routing to eliminate the radius, but I need to keep it at a minimum.
>
> Thanks in advance for your input.
>
> David Baldwin C.I.D.+
>
>
> ---------------------------------------------------------------------------------
> DesignerCouncil Mail List provided as a free service by IPC using LISTSERV
> 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF DesignerCouncil.
> To temporarily stop/(restart) delivery of DesignerCouncil send: SET
> DesignerCouncil NOMAIL/(MAIL)
> Search previous postings at: www.ipc.org > On-Line Resources & Databases >
> E-mail Archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16for additional information, or contact Keach Sasamori at
> [log in to unmask] or 847-615-7100 ext.2815
>
> ---------------------------------------------------------------------------------
>
---------------------------------------------------------------------------------
DesignerCouncil Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF DesignerCouncil.
To temporarily stop/(restart) delivery of DesignerCouncil send: SET DesignerCouncil NOMAIL/(MAIL)
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
---------------------------------------------------------------------------------
|
|
|