Indeed strange. Very few crystals have this acicular form, except metal
whiskers. My first reaction is have them analysed!
Brian
Davis, Larry wrote:
> We have a strange problem here and I was hoping someone could provide an
> explanation. I had Steve post a couple pictures to his site for
> viewing, thanks Steve!
>
> We are seeing this crystalline growth all over a single assembly that
> was built back in Feb 07 and shipped to one of our customers who kept it
> stocked in the original esd bag. They noticed it once it was required
> for use and returned it to us. The only thing in our process that I
> think could possibly be the root cause is that our board cleaner solvent
> (Bioact EC-7R) was getting very flux loaded about that time but we
> haven't seen this on any other assemblies that have been built since
> then. We are using no-clean fluxes and only clean boards that have high
> impedance circuitry. I find it very strange that the growth occurs on
> the plastic parts as well as the leads of components. Any ideas?
>
> http://stevezeva.homestead.com/files/crystal_growth.jpg
>
> http://stevezeva.homestead.com/files/crystal_growth_closeup.jpg
>
>
> Thanks in advance for your feedback!
>
> Larry Davis
> Hach Co.
>
>
> This message (including any attachments) contains confidential
> and/or proprietary information intended only for the addressee.
> Any unauthorized disclosure, copying, distribution or reliance on
> the contents of this information is strictly prohibited and may
> constitute a violation of law. If you are not the intended
> recipient, please notify the sender immediately by responding to
> this e-mail, and delete the message from your system. If you
> have any questions about this e-mail please notify the sender
> immediately.
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|