We have a strange problem here and I was hoping someone could provide an
explanation. I had Steve post a couple pictures to his site for
viewing, thanks Steve!
We are seeing this crystalline growth all over a single assembly that
was built back in Feb 07 and shipped to one of our customers who kept it
stocked in the original esd bag. They noticed it once it was required
for use and returned it to us. The only thing in our process that I
think could possibly be the root cause is that our board cleaner solvent
(Bioact EC-7R) was getting very flux loaded about that time but we
haven't seen this on any other assemblies that have been built since
then. We are using no-clean fluxes and only clean boards that have high
impedance circuitry. I find it very strange that the growth occurs on
the plastic parts as well as the leads of components. Any ideas?
http://stevezeva.homestead.com/files/crystal_growth.jpg
http://stevezeva.homestead.com/files/crystal_growth_closeup.jpg
Thanks in advance for your feedback!
Larry Davis
Hach Co.
This message (including any attachments) contains confidential
and/or proprietary information intended only for the addressee.
Any unauthorized disclosure, copying, distribution or reliance on
the contents of this information is strictly prohibited and may
constitute a violation of law. If you are not the intended
recipient, please notify the sender immediately by responding to
this e-mail, and delete the message from your system. If you
have any questions about this e-mail please notify the sender
immediately.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|