It depends (Whittaker Trade Mark). John Burke, the spokesman for making
electronics as cheap and fast and simple as possible, may tell you this: If
your product is for the cheapest of cheap parabola antennas, or for a simple
home LAN, use the cheapest FR-4 or paper board you can find. Such products
are so uncritically designed, that anything will work.
On the other hand, if your customer is a responsible and demanding company
in Germany, you should not even use the word cheap, but be anxious to
fulfill the customer's requirements plus little extra.
The interpretation of what is said above is yours, I take no responsibility
for the content of the first part.
Inge
PS. Duroid, Taconic, Arlon, Speedboard...whatever they call themselves, they
seem to be approximately the same. We have been looking for a real low-cost
microwave material for years, and found none. One way to bring down the cost
is to plan the design in a way, that you can use FR4 as much as possible,
and microwave board material on such little area as possible. Many years
ago, we even planned to buy the ingredients and laminate microwave boards
ourselves!
-----Ursprungligt meddelande-----
Från: TechNet [mailto:[log in to unmask]] För Marsico, James
Skickat: den 7 augusti 2007 20:36
Till: [log in to unmask]
Ämne: [TN] Microwave Laminate Material
Hello Technet:
I'm looking for recommendations for a low cost microwave laminate with a
dielectric constant of about 3 and a dissipation factor of about .001.
I believe Taconic RF-30 is pretty reasonable, but is there anything out
there that might be less?
Jim Marsico
EDO Corporation
Amityville: 631-630-5079
Bohemia: 631-218-7057
[log in to unmask]
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|