I already had and was weighing the somewhat colorful nature of my reply and its impact on the delicate sensibilities of the audience, when I saw your and Inge's response. I laughed out loud so never mind.
All good answers so far. After you have verified proper temperatures and chemistries of you cleaning equipment/process and are still having a problem, vary the product loading. Put fewer assemblies in that have been exposed to the same flux chemistries and space them apart. This will validate whether you are exceeding the capacity of your equipment/process.
All the other answers become more complex and may not be solved without the use of some structured DOEs.
Dewey
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Brian Ellis
Sent: Tuesday, August 14, 2007 12:34 AM
To: [log in to unmask]
Subject: Re: [TN] Aqueous batch cleaner foaming
I think Dewey will answer that!
Soft soap is made from potassium hydroxide and vegetable oils (notably
olive oil). It must not contain any salt or cosmetic additives, such as
colouring matter or perfumes. It is sold in pharmacies and is used for
the treatment of some skin conditions. It is milder than hard soap (what
you usually see), which is made from sodium hydroxide and has added salt
to harden it.
Brian
Hernefjord Ingemar wrote:
> soft white soap, what's that?
> Inge
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Brian Ellis
> Sent: den 14 augusti 2007 09:05
> To: [log in to unmask]
> Subject: Re: [TN] Aqueous batch cleaner foaming
>
> I agree with Rudy, especially about temperature. However, if your first water is too hot, depending on the flux chemistry, the cleaning quality may be less good. This is especially so if the flux activator contains amino acids or their derivatives. The ideal temperature is 55-60°C, no higher.
>
> You can buy defoamer from flux manufacturers, but add minimal quantities. This is not a case of a little is good, so a lot must be better. Alternatively, you can make your own. I quote my book:
> "Dissolve 300 g soft white soap in one litre of hot water. When cool, add one litre of octyl alcohol. Shake before use. Add the minimum dose to obtain the desired effect, usually about 0.1 cm3/l"
>
> Brian
>
> Rob Strecker wrote:
>> All,
>>
>> Has anyone else had foaming issues in an aqueous wash batch cleaner?
>> What are some of the causes of excess foaming? We are applying our
>> wave flux via spray; however this flux is also suitable in foaming
>> flux applications. We are currently in the process of optimizing our
>> flux application in the wave to significantly reduce the flux residue
>> on the boards. This includes optimizing the sprayers, preheats and dwell time.
>> Initial tests show this is not having a major impact in reducing the
>> foaming. We will be testing boards with only SMT flux residue, then
>> ones with only wave flux residue. The theory is that by themselves
>> they do not foam but when mixed cause foaming. We have recently
>> changed Paste suppliers, thus we now have two different manufactures
>> of flux mixing in the wash (one from SMT, one from wave). Could this
>> be a cause of excessive foaming?
>>
>>
>>
>> Thanks,
>>
>> Rob Strecker
>>
>>
>> ---------------------------------------------------
>> Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
>> unsubscribe, send a message to [log in to unmask] with following text in
>> the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt
>> or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET
>> Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
>> posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
>> archives of previous posts at: http://listserv.ipc.org/archives Please
>> visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>> for additional information, or contact Keach Sasamori at
>> [log in to unmask] or 847-615-7100 ext.2815
>> -----------------------------------------------------
>>
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|