Hi QiXiong,
For the question 1, I saw IPC-SM--782A which has its recommendation. It
is 0.5mm. same for both resistor and cap chip. << see sec 8.1, clause
5.0, sec 8.2, clause 5.0)
Basically, IPC is more conservative in the design
I also refer some experimental result for other dimension of chip pad
0201 Spacing (Universal company - experiment) - 6 - 8 mil spacing
01005 Spacing (Alpha Metals) - 3 mil spacing
Jackson Chan
Technical Services Manager
Cookson Electronics - Alpha metals
From: TGAsia [mailto:[log in to unmask]] On Behalf Of Liu Qixiong
Sent: Thursday, August 09, 2007 8:23 AM
To: [log in to unmask]
Subject: [TGA] 请教PCB板变形&焊盘设计
Dear all,
早上好!
目前遇到2个问题,有些疑问,需要各位给出些建议:
1)我们遭遇到连锡,发现PCB板0805与0402焊盘间距离有0.22mm,分析为焊盘间最小
设计安全
距离为0.3mm,否则,会有焊点间会有牵引力,小元件就会被拉近大元件,形成偏位
或连锡。
从IPC标准上查,发现有光板导体间安全电气距离为0.13mm,(IPC-2221 表
6-1),没有关
于焊盘设计的安全距离,不知有其他IPC标准规定?另牵引力的分析,是否有理论依
据?
象这种情况,如果PCB焊盘设计更改困难,有否其他工艺方法改善?
2)生产线PCB板尺寸为190x155mm,厚度有1.04mm,有1BGA尺寸偏大 30x30mm(焊点
26x26),
在返修BGA台返修时,发现PCB板很容易变形,弓曲变形80%超过0.75%的标准
(IPC-A-610D 10.2.7)
不知有无好的工艺方法能避免PCB板变形?
因刚加入这个组织,也许之前有讨论过,还请多多包涵。
以上,非常感谢。
Thanks and Best regards,
QiXiong Liu / 刘启雄
*******************************************
Shenzhen Kaifa Tech. Co., Ltd
TEL:(86-755) 8303 2489 Ext: 33489
HP: 13480838497
E-MAIL:[log in to unmask]
*******************************************
This message has been scanned.
(210.245.235.14)
Legal Disclaimer: The information contained in this message may be
privileged and confidential. It is intended to be read only by the
individual or entity to whom it is addressed or by their designee. If the
reader of this message is not the intended recipient, you are on notice
that any distribution of this message, in any form, is strictly prohibited.
If you have received this message in error, please immediately notify the
sender and delete or destroy any copy of this message
|
|
|