I also feel that it is something that the entire surface was exposed to
since they are growing on everything including plastics and the
laminate. I've inspected the inside of the bags and they do not exhibit
any type of crystal growth nor do they have any kind of residues. The
bags were brand new before these assemblies were placed into them.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Dennis Fritz
Sent: Wednesday, August 01, 2007 10:37 AM
To: [log in to unmask]
Subject: Re: [TN] Strange crystal growth
In a message dated 8/1/2007 10:21:32 A.M. Eastern Daylight Time,
[log in to unmask] writes:
the growth occurs on
the plastic parts as well as the leads of components. Any ideas?
Can you supply details on the component leads? But if it is on the
plastic, also, that would mean it is something that the entire surface
of the assembly has been exposed to. Any chance there is something on
the inside of the bag being transferred to the assembly? Antistat?
Denny Fritz
MacDermid.
************************************** Get a sneak peek of the all-new
AOL at http://discover.aol.com/memed/aolcom30tour
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
This message (including any attachments) contains confidential
and/or proprietary information intended only for the addressee.
Any unauthorized disclosure, copying, distribution or reliance on
the contents of this information is strictly prohibited and may
constitute a violation of law. If you are not the intended
recipient, please notify the sender immediately by responding to
this e-mail, and delete the message from your system. If you
have any questions about this e-mail please notify the sender
immediately.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|