TECHNET Archives

August 2007

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Wed, 8 Aug 2007 10:57:12 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Kane, Amol (349)" <[log in to unmask]>
Subject:
From:
"Kane, Amol (349)" <[log in to unmask]>
MIME-Version:
1.0
In-Reply-To:
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
Parts/Attachments:
text/plain (387 lines)
A tangent to the original question on rework...........what are arguments for and against reflowing an entire assembly (putting it thru the reflow oven again) instead of reworking say 4 or 5 BGAs on the same board by traditional BGA rework equipment?

True, all the other components (including the good BGAs) will undergo one more reflow....but are there studies/literature out there that suggest that this induces failures among earlier good and working components?

If there is a choice between subjecting the board to 4X2=8 thermal cycles for removal and replacement of the 4 BGAs (scrapping the board is not an option), reflowing the entire assembly once makes sense.

Am I missing some important consideration/s here?

Thanks,

Amol

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of David D. Hillman
Sent: Wednesday, August 08, 2007 10:45 AM
To: [log in to unmask]
Subject: Re: [TN] Rework question

Hi gang! As many folks have pointed out, there is no IPC
guideline/specification that contains a maximum rework limit value. I have
two additional considerations when attempting to create a maximum rework
limit value - the laminate Tg in relation to the solder process and the
laminate CTE value above the Tg value (typically designated as alpha 2).
If your soldering process exceeds the laminate Tg then you are inducing a
significant amount of stress on pwa structures such as pads, traces, and
plated thru holes - the higher the laminate Tg value, the lower  the
amount of induced stress (or alternatively, a soldering process
temperature below the laminate Tg would be good). Also, if the CTE value
above the Tg is high, then the time duration above the Tg for the rework
process should be minimized as much as possible. The pwa laminate is a
critical consideration of the maximum rework limit value thus the reason
for not finding an IPC recommendation - "it depends" on the laminate used.

And Dewey - handing Doug a soldering iron is like asking me to spray
conformal coating - a really bad idea!

Dave Hillman
Rockwell Collins
[log in to unmask]




"Whittaker, Dewey (EHCOE)" <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
08/07/2007 01:22 PM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
"Whittaker, Dewey (EHCOE)" <[log in to unmask]>


To
[log in to unmask]
cc

Subject
Re: [TN] Rework question






Excellent points made by Bev and yourself and I concur. The answer to
one of the initial questions was whether there were a different number
of reworks allowed if it was a Lead-free process or not. For the
Aerospace Industry, if and when we are Lead-free the assemblies will
have to be equal to or better than the current leaded processes, so
there would be no difference in the reworks allowed.
As a precursor to that happening our laminate materials we specify now
are already being tested to those processing conditions and end use
environments. The designs are robust enough that there is no potential
limit to the number of thermal excursions they can experience under
controlled conditions. I have tried to make the printed boards
bullet-proof so no matter who it is outsourced to for the assembly
portion, they will meet the expected performance requirements. They
should even tolerate being soldered by Doug Pauls.
Dewey

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard D.
Sent: Tuesday, August 07, 2007 10:59 AM
To: [log in to unmask]
Subject: Re: [TN] Rework question

I thought so. How could something like that be applied, as Bev correctly
pointed out. There are too many variables that would determine the
number of "safe" reworks.
I prefer the term "Tg excursions" when a rework limit is set on
agreement with customer and supplier. And a careful qualification is
needed, as Bev pointed out, and it is usually a worthwhile effort to do
so. Solder touchup and hand-soldering are usually excluded from this
number, as this type of rework seldom leads to reliability issues. But
again, there are exceptions.
In addition to having "seen thin boards delaminated after a single, poor
attempt at rework" I have also seen any given size and thickness and
material type delaminated in spite of very careful qualification of the
rework process. Also, I have seen Z-axis expansion as a result of too
large of a delta T between the localized rework site and the rest of the
assembly cause damage to vias and PTH barrels that went totally
undetected by a careful inspection and X-ray and electrical test,
including stress screening, only to fail later.
This is why the hard limitation of the number of reworks was deleted
when the standards changed from WS6536E, to J-STD-2000, to today's
J-STD-001D and IPC-A-610D. There is no number of Tg excursions that is
"safe" for every application.



-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Bev Christian
Sent: Tuesday, August 07, 2007 12:09 PM
To: [log in to unmask]
Subject: Re: [TN] Rework question

Same here.
Bev
RIM

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of John Burke
Sent: Tuesday, August 07, 2007 12:55 PM
To: [log in to unmask]
Subject: Re: [TN] Rework question

Just looked in 7711 - didn't see a reference to it...

John



John Burke

(408) 515 4992

-----Original Message-----
From: Guy Ramsey [mailto:[log in to unmask]]
Sent: Tuesday, August 07, 2007 9:14 AM
To: 'TechNet E-Mail Forum'; 'John Burke'
Subject: RE: [TN] Rework question

I don't think it is worded as a hard limit. Might be IPC-7711.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of John Burke
Sent: Tuesday, August 07, 2007 12:04 PM
To: [log in to unmask]
Subject: Re: [TN] Rework question

The question actually came up because there is stated (somewhere?) in an
IPC document the number of reflow cycles you are allowed to put the
board through.

Taking that limit into account (first side reflow, second side etc)
allowed them to remove and replace the same component 3 times in a worst
case scenario.

And I agree with Bev the whole thing is open to interpretation as to
what represents a reflow cycle - pad dressing removal etc.




John Burke

(408) 515 4992
-----Original Message-----
From: Bev Christian [mailto:[log in to unmask]]
Sent: Tuesday, August 07, 2007 8:53 AM
To: TechNet E-Mail Forum; John Burke
Subject: RE: [TN] Rework question

John,
I am having people look, but if there is a limit I do not remember.
However, from a practical point of view, the answer is Doug Pauls'
patented (Or is that copyrighted or trade marked? Being a lawyer, I
don't
know.) phrase, "It all depends".  It depends on the method of rework,
(reflow, wave solder, selective soldering, soldering iron, hot air gun
focused IR, flame), temperatures reached, ramp rates, dwells, size of
board, thickness of board, type of component, heat sinks, skill of
operator. I could go on.  Make yourself a fishbone diagram.

And then are we talking about say 3X of the same component, or 5X
side-by-side or 7x but each in a thermally separated area from the other
six?

Here's a scenario for you: double sided reflow and then required rework
under cans on both sides of the board. So this means two more for can
removal, dressing the can pads, removing the components, dressing the
pads, part deposition, can replacement.  And hope everything works!

So you need visual inspection, x-ray inspection, electrical test and if
you really want to do it right, x-sectioning and a whole battery of
reliability testing.

I have seen good work and I have seen thin boards delaminated after a
single, poor attempt at rework.

Bev
RIM

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of John Burke
Sent: Tuesday, August 07, 2007 10:29 AM
To: [log in to unmask]
Subject: [TN] Rework question

Hi,



I had a question yesterday which was "has the number of re-work cycles
allowed by IPC changed for lead free?"



And I confess I don't know but I bet someone on this link does.



If you could let me know number of thermal cycles allowed and the spec
reference I would be grateful.



John







John Burke



(408) 515 4992




---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential
information, privileged material (including material protected by the
solicitor-client or other applicable privileges), or constitute
non-public information. Any use of this information by anyone other than
the intended recipient is prohibited. If you have received this
transmission in error, please immediately reply to the sender and delete
this information from your system. Use, dissemination, distribution, or
reproduction of this transmission by unintended recipients is not
authorized and may be unlawful.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential
information, privileged material (including material protected by the
solicitor-client or other applicable privileges), or constitute
non-public information. Any use of this information by anyone other than
the intended recipient is prohibited. If you have received this
transmission in error, please immediately reply to the sender and delete
this information from your system. Use, dissemination, distribution, or
reproduction of this transmission by unintended recipients is not
authorized and may be unlawful.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------



CONFIDENTIALITY NOTICE: 
This e-mail, and any attachments, is for the sole use of the intended 
recipient(s) and may contain information that is confidential and 
protected from disclosure under the law. Any unauthorized review, use, 
disclosure, or distribution is prohibited. If you are not the intended 
recipient, please contact the sender by reply e-mail, and delete/destroy 
all copies of the original message and attachments. 
Thank you.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2