TECHNET Archives

August 2007

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
"Wenger, George M." <[log in to unmask]>
Date:
Fri, 10 Aug 2007 20:49:06 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Cheryl Tulkoff <[log in to unmask]>
Content-type:
text/plain; charset=US-ASCII
Subject:
From:
Cheryl Tulkoff <[log in to unmask]>
X-cc:
TechNet E-Mail Forum <[log in to unmask]>
In-Reply-To:
MIME-Version:
1.0
Parts/Attachments:
text/plain (241 lines)
George -

Enthone calls is "copper creep". It is also referred to as copper
corrosion. Dave Hillman of Rockwell published on it.

http://www.smta.org/knowledge/proceedings_abstract.cfm?PROC_ID=1765

The HP paper was presented at ISFTA 2006:
(See attached file: S18_1.pdf)

Unfortunately, you've caught me on the road at the moment. I can send you
further docs and pics next week when I have access to the rest of my
material.

Thanks,
Cheryl Tulkoff
Senior Reliability Engineer
Phone:(512) 683-8586
Fax: (512) 683-8520
National Instruments
11500 N. Mopac Expressway
Building C
Austin, TX 78759-3504




                                                                           
             "Wenger, George                                               
             M."                                                           
             <George.Wenger@an                                          To 
             drew.com>                 "TechNet E-Mail Forum"              
                                       <[log in to unmask]>, "Cheryl Tulkoff" 
             08/10/2007 07:30          <[log in to unmask]>             
             PM                                                         cc 
                                                                           
                                                                   Subject 
                                       RE: [TN] Silver PCB finish and      
                                       reliability (question)              
                                                                           
                                                                           
                                                                           
                                                                           
                                                                           
                                                                           




Cheryl,

When you indicate a quick Google search on the topic, what topic are you
referring to?  Copper creep is typically a thermal issue with copper
alloys and I'm not sure I've every seen it related to immersion silver
surface finish.

Regards,
George
George M. Wenger
Andrew Corporation Wireless Network Solutions
Senior Principal FMA / Reliability Engineer
40 Technology Drive, Warren, NJ 07059
(908) 546-4531 [Office]  (732) 309-8964 [Cell]

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Cheryl Tulkoff
Sent: Friday, August 10, 2007 6:30 PM
To: [log in to unmask]
Subject: Re: [TN] Silver PCB finish and reliability (question)

Carl -

Immersion silver is our finish of choice for most of our PCBs - both
leaded
and lead free. There is one known reliability issue referred to as
"copper
creep." In customer environments with high sulfur along with humidity
and
air flow, you can get catastrophic failures. This usually affects vias
or
other areas where there is no solder over the silver. Both Dell and HP
have
published on the topic and we have confirmed failures due to the problem
as
well. We have been working with the immersion silver finish suppliers on
potential improvements.

Industries like tire manufacture, water treatment, paper processing etc.
are likely candidates for problems.

You can do a quick google search on the topic. If you cannot locate the
papers, you can contact me for more details.

Cheryl Tulkoff
Senior Reliability Engineer
Phone:(512) 683-8586
Fax: (512) 683-8520
National Instruments
11500 N. Mopac Expressway
Building C
Austin, TX 78759-3504






             Carl VanWormer

             <[log in to unmask]>

             Sent by: TechNet
To
             <[log in to unmask]>         [log in to unmask]


cc


             08/10/2007 04:07
Subject
             PM                        [TN] Silver PCB finish and

                                       reliability (question)



             Please respond to

              TechNet E-Mail

                   Forum

             <[log in to unmask]>

             ; Please respond

                    to

              Carl VanWormer

             <[log in to unmask]>









For non-BGA, surface mount boards, we have always ordered HASL boards.
In
our progress towards ROHS compliance, management has changed the default
specification to ENIG.  Our board house has HASL, ENIG, and Silver as
options, with Silver at about the same price as HASL and ENIG with a
significant premium (along with a 2 to 3 days added to the processing
time).  When I asked management why we couldn't use Silver, I was told
that
there are significant problems with the Silver processed boards (with no
real explanation).

My question to the Group:  Is there any good reason to avoid Silver as a
surface finish on my consumer and industrial boards?

Your scary stories are welcomed . . .

Thanks,
Carl





Carl Van Wormer
Cipher Systems
1800 NW 169th Place, Suite B-100
Beaverton, OR  97006
Phone (503)-617-7447 extension 20




---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------


------------------------------------------------------------------------------------------------

This message is for the designated recipient only and may
contain privileged, proprietary, or otherwise private information.
If you have received it in error, please notify the sender
immediately and delete the original.  Any unauthorized use of
this email is prohibited.
------------------------------------------------------------------------------------------------

[mf2]


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2