Blair
Try installing a dehumidifier in the coating area - cheaper than A/C.
The haze is almost certainly trapped moisture in the coating giving
it a somewhat dull appearance. Of course do first check your air-line
filters to be sure thy aren't clogged with water...
Kindest regards,
Graham Naisbitt
[log in to unmask]
On 27 Jul 2007, at 19:48, Hogg, Blair K. wrote:
> Technetters,
>
> We spray some of our conformally coated boards by hand and air dry
> them.
> The area used for this is not air conditioned and during humid
> times we
> sometimes see boards with a hazy appearance. Any thoughts on how we
> can
> correct this, other than air conditioning the spray booth?
>
> Thanks,
>
> Blair
>
> *******************************************************************
> This email and any files transmitted with it are confidential and
> intended solely for the use of the individual or entity to whom they
> are addressed. If you have received this email in error please notify
> the system manager.
>
> This footnote also confirms that this email message has been swept
> for the presence of computer viruses.
>
> www.Hubbell.com - Hubbell Incorporated
>
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following
> text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail
> to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/
> archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?
> Pageid=4.3.16 for additional information, or contact Keach Sasamori
> at [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|