Blair
If the soldermask thickness conforms to the IPC spec it should be adequate.
What may be occurring is pin holes in the soldermask or contaminants either
on the board prior to soldermask or if the board is HASLed flux residues.
Best regards
Lee
J. Lee Parker, Ph.D.
JLP Consultants LLC
804 779 3389
----- Original Message -----
From: "Hogg, Blair K." <[log in to unmask]>
To: <[log in to unmask]>
Sent: Thursday, July 05, 2007 11:37 AM
Subject: [TN] Soldermask Thickness
We switched PC board suppliers for one of our products a while back and
have started having hipot issues with components that are connected to
main 110VAC input voltage arcing through the soldermask to tracks
underneath at 1200V hipot voltage.
I'm pretty sure I'll get a few responses that say that we shouldn't be
using the soldermask as an insulator, however, since the change in
supplier seems to coincide with the onset of problems, I've been asked
to evaluate the soldermask thickness as a potential contributor to the
problems.
I would some recommendations on how to measure the thickness of the
soldermask.
Thanks,
Blair
*******************************************************************
This email and any files transmitted with it are confidential and
intended solely for the use of the individual or entity to whom they
are addressed. If you have received this email in error please notify
the system manager.
This footnote also confirms that this email message has been swept
for the presence of computer viruses.
www.Hubbell.com - Hubbell Incorporated
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|