Lu, Angela,您好!



	  可能与PCB绿油粘附力不良有关。



======= 2007-07-25 15:41:22 您在来信中写道:=======



> 

> 

>大家好,

> 

>   现在遇到个棘手的问题,车间在用电动螺丝刀,在标准的扭力要求下,打螺丝时,把边缘的绿油脱落了,由于此板螺丝的用量是24个,现在已做了近50片的产量,几乎每片每个都是如此现象,导致我们现在也停产了,能否告知是什么原因导致此不良现象?我们也正在与裸板的供应商联系,可是仍没有给出明确的答复。谢谢各位大侠们的帮助。  有什么弥补的办法吗? 

> 

> 

> 

> 

> 

> 

> 



= = = = = = = = = = = = = = = = = = = =

			



        致

礼!

 

				 

贺光辉        



中国赛宝实验室可靠性研究分析中心

地址:广州市东莞庄路110号

邮编:510610

电话:020-87236986

邮箱:[log in to unmask]

2007-07-25