Not exactly. A laser beam is used to burn away the surface material to a
certain depth.
Color contrast can be obtained by using colored materials. An example is
green solder mask etched away to expose bright yellow fiberglass
underneath, or etching a metal with a black anodized surface to expose
the shiny stainless steel underneath, etc.
Lasers can be used to etch extremely detailed graphics onto the surface,
in addition to the common bar codes and alphanumeric information.
When using laser etch, one needs to understand that the reader of the
etched information must be able to read the contrast between the two
mediums, whether it is an infrared scanner or the human eye. Usually the
problems with reading the laser-etched information is in the ability of
the reading device to discern the difference in contrast, not the
accuracy of the laser etching itself. The legibility is in the level of
contrast.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Kevin Glidden
Sent: Wednesday, July 25, 2007 9:23 AM
To: [log in to unmask]
Subject: Re: [TN] Laser marking for PWBs
Are laser markers capable of color (red / black / white) as well?
Kevin Glidden
Manufacturing Engineer
Luminescent Systems Inc.
-----Original Message-----
From: Whittaker, Dewey (EHCOE) [mailto:[log in to unmask]]
Sent: Wednesday, July 25, 2007 9:51 AM
To: [log in to unmask]
Subject: Re: [TN] Laser marking for PWBs
Yes, sold them and went to machine readable code labels.
Dewey
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard D.
Sent: Wednesday, July 25, 2007 5:36 AM
To: [log in to unmask]
Subject: Re: [TN] Laser marking for PWBs
Thank you! Any others care to respond on their experiences with laser
markers?
-----Original Message-----
From: Gumpert, Ben [mailto:[log in to unmask]]
Sent: Wednesday, July 25, 2007 6:16 AM
To: Stadem, Richard D.; TechNet E-Mail Forum
Subject: RE: Laser marking for PWBs
I wasn't too involved in the process, but we recently procured and are
using a system from Control Micro Systems
(http://www.cmslaser.com/pcb/html/pcbmarking.php). We validated its use
on a variety of board types and other materials. It's CO2, so it won't
etch metals, but if needed, a coat of ink can be applied to metal
surfaces which is then permanently 'cured' on where hit by the laser.
Ben
-----Original Message-----
From: Stadem, Richard D. [mailto:[log in to unmask]]
Sent: Wednesday, July 18, 2007 2:35 PM
Subject: Laser marking for PWBs
Hi folks,
I am looking at purchasing a laser marking system for the purpose of
laser etching the board serial number, part number, etc.
I have little experience with this type of process, and which systems
are better than others, etc.
Any feedback you care to share with me? Labels and ink stamping are not
an option in this case.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|