Thanks, Peter, you are right.
Your help will be appreciated; I would like to have a try. BTW, the problem we are facing is not only 10 pcs component, but 10 items with thousands of pcs each one. It may benefit a lot.
I am looking forward further information.
Sky He
GE Business Account
Jabil Circuit(Shanghai) Ltd.
Tel: +86-21-64858585*1815
Mobil: +86-1376-4317-858
Fax: +86-21-54261228
-----Original Message-----
From: Deng, Peter (Shenzhen) [mailto:[log in to unmask]]
Sent: 2007年7月18日 1:27
To: Asia Committe Task Group Forum; Sky He
Subject: RE: [TGA] Restore component solderability of last time buy!
Dear Sky,
Perhaps you got information by ACI, I don't know whether there is local Chinese vendor or business organization to provide similar service.
Maybe Harbin Institute of Technology would like to try; if you really need we can help to coordinate but I think it can't reduce your lost compared with service cost if sample is only 10 components.
Peter Deng
**************************************************
Reliability Lab
Electrical & Electronics
Consumer Testing Services
SGS Shenzhen branch
Tel + 86 0755-26710624
Mobile + 86 13828768267
Fax + 86 0755-26710594
Email [log in to unmask]
Website www.sgs.com/ee
-----Original Message-----
From: TGAsia [mailto:[log in to unmask]] On Behalf Of Sky He
Sent: 2007年7月17日 8:52
To: [log in to unmask]
Subject: [TGA] Restore component solderability of last time buy!
Friends,
We got a problem that we have several (about 10) components that have
poor solderability and coplanarity due to excessive age.(old date code)
We must use the parts because they are out of production - Last Time
Buy.
I heard that there is a service call ROSA (Reduced Oxide Solderability
Activation) to remove metal oxides and sulfides that inhibit
solderability. It can be performed on tin oxides, copper oxides, silver
oxides, and silver sulfides. This technique is excellent for components
and boards that had not been stored properly and exhibit poor
solderability.
Do anyone know if there is a Chinese vendor can perform this?
PS: The parts are in trays (waffle pack) - Quad Flat Pack and PQFP.
Sky He
GE Business Account
Jabil Circuit(Shanghai) Ltd.
Tel: +86-21-64858585*1815
Mobil: +86-1376-4317-858
Fax: +86-21-54261228
Information in this email and any attachments is confidential and
intended solely for the use of the individual(s) to whom it is addressed
or otherwise directed. Please note that any views or opinions presented
in this email are solely those of the author and do not necessarily
represent those of the Company.
Finally, the recipient should check this email and any attachments for
the presence of viruses. The Company accepts no liability for any damage
caused by any virus transmitted by this email.
All SGS services are rendered in accordance with the applicable SGS
conditions of service available on request and accessible at
http://www.sgs.com/terms_and_conditions.htm
|
|
|