not sure if this helps.
http://www.smtsz.com/download/qxjfycs.pdf
Hermus Leung
Technical Service Engineer, 3M Hong Kong
Victoria Centre, 5/F., 15, Watson Road, Hong Kong
Fax : (852) 2969-5758
Tel : (852) 2806-6407
eMail : [log in to unmask]
"Yu, Gary"
<gary.yu@VIASYSTE
MS.COM> To
Sent by: TGAsia [log in to unmask]
<[log in to unmask]> cc
Subject
07/30/2007 11:23 Re: [TGA] 请教E8=AF=B7=E6=95=99 ?=
PM
Please respond to
Asia Committe
Task Group Forum
<[log in to unmask]>;
Please respond to
"Yu, Gary"
<gary.yu@VIASYSTE
MS.COM>
CAF is a complex issue, not just a material issue. Even the base material
have Anti-CAF, if PCB fabricator did not well control their process, it
also fail in CAF testing.
Best regards,
Gary Yu
-----Original Message-----
From: TGAsia 代理 [log in to unmask]
Sent: 30/7/2007 [Mon] 22:28
To: [log in to unmask]
Cc:
Subject: Re: [TGA] 请教E8=AF=B7=E6=95=99?=
个人认为非CAF材料未开纤作Migration测试意义不大,大家谈的测试
条件应该满足CUSTOMER COUPON,IPC STD中有SIR TEST COUPON 可参考,
另测试条件应该附加测试电压DC100 or 50V,加速Cu离子迁移.
winsun zhao/赵文成
在2007-07-26,"JiaXing LIU" <[log in to unmask]> 写道:
大家也好
我们也有同样的CAF问题。
请问如果用的是普通的非CAF材料,PTH孔的间距最小安全
间距是多少不会有CAF的问题?如果用
anti-CAF的材料的话,PTH孔的间距最小安全间距是多
少?
Isola 370HR, Tg>=150degrees, Td 340D. core
thickness is 0.7mm, 2X7628
core. Total thickness is 1.6mm, 1Oz Copper.
8 pairs of via holes with 15.7mils parallel
distance between hole wall
to hole wall. The pair of holes is anode and
cathode.
The hole size is 0.35mm. finish is immersion
silver.
我们的测试要求是85度和85%湿度, 1000小
时.
>>> Li Ruijuan <[log in to unmask]> 2007-7-26
11:23 >>>
大家好!
请问关于PCB板过孔之间的绝缘阻抗要求是什么,测试条件
呢,对孔距\孔径有没有要求
?另外,如果验证是否会有CAF缺陷,实验条件怎样规定,谢
谢
孔间距很大,湿热试验后孔间绝缘电阻却减小很多,可能是
什么原因呢?
--------------------------------------------------------
ZTE Information Security Notice: The information
contained in this mail
is solely property of the sender's organization.
This mail communication
is confidential. Recipients named above are
obligated to maintain
secrecy and are not permitted to disclose the
contents of this
communication to others.
This email and any files transmitted with it are
confidential and
intended solely for the use of the individual or
entity to whom they are
addressed. If you have received this email in
error please notify the
originator of the message. Any views expressed in
this message are those
of the individual sender.
This message has been scanned for viruses and Spam
by ZTE Anti-Spam
system.
_____
《大 话 西 游 3》 首 届 玩 家 见 面 会 即 将 在 广 州 召
开!敬 请 关 注 >> <http://event.mail.163.com/chanel/xy3.htm?from=126_NO9>
|