Same here we used alcohol to remove the residue. Ultimately your profiling process should burn off all the flux. You might want to re-check that process as well.
Ronald D. Peeler Jr., B.S. IE
Process Engineer
SWEMCO
Moorestown, NJ 08057
Tel: (856).222.9900 ext. 31
Cel: (484).948.0779
Fax: (856).222.0700
[log in to unmask]
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of [log in to unmask]
Sent: Wednesday, July 11, 2007 3:02 PM
To: [log in to unmask]
Subject: Re: [TN] No Clean flux residue after water wash
Yes, I have experienced this issue and found that using a saponifer or alcohol removed the residues.
Kat
----- Original Message -----
From: "Tom P. Hummel" <[log in to unmask]>
Date: Wednesday, July 11, 2007 1:50 pm
Subject: [TN] No Clean flux residue after water wash
To: [log in to unmask]
> Fellow TechNetters,
>
>
>
> We are experiencing a white residue on the solder side of some boards
> after going through our wash system. We are wave soldering the boards
> on a SeHo wave solder machine using Aim NC-264-5 no clean flux. The
> boards have some additional components installed by hand using water
> soluble flux/solder. The boards are then run through our Aqueous
> Technologies SMT series board washer. When they complete the drying
> cycle, there is a white residue on the solder side of the boards
> that is
> very difficult to remove. Has anyone else seen this residue from
> washing a board after using no clean flux? Does anyone have any
> recommendations to help eliminate the residue?
>
>
>
>
>
> Thomas P. Hummel
>
> Carlton Industries Corp
>
>
>
>
>
>
>
>
>
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following
> text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail
> to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
> http://listserv.ipc.org/archivesPlease visit IPC web site
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-
> 615-7100 ext.2815
> -----------------------------------------------------
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|