TECHNET Archives

July 2007

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Tue, 10 Jul 2007 09:22:03 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Kane, Amol (349)" <[log in to unmask]>
Subject:
From:
"Kane, Amol (349)" <[log in to unmask]>
MIME-Version:
1.0
In-Reply-To:
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
Parts/Attachments:
text/plain (116 lines)
Dear Technetters,
We are seeing dull SMT solder joints near some TH parts that go over the wave. The board top side temp is getting to 110C. using OA flux at wave and SMT. The boards are immediately put thru an aqueous wash. The SMT joints were shiny coming out of SMT. The customer is noticing this because other areas of the board (except near the TH parts) look shiny.
There are no residues on the joints as I tried to manually clean a joint with water and IPA and did not have any flux residue on the Q-tip.

Has anybody else noticed this phenomenon?......the only literature I could find on dull SnPb joints says the dull appearance could be due to a "cold" joint, which I know is not the case. Even though this is not a defect I want to know the reason for this to happen.

Could the wave flux cause this issue?

Amol

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Bev Christian
Sent: Tuesday, July 10, 2007 8:19 AM
To: [log in to unmask]
Subject: Re: [TN] Injury by array

Jeff,
Two other possibilities (both costing $) are:
1) automatic board handler
2) gloves

I don't like either one, but there they are.
Bev
RIM

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of McGlaughlin, Jeffrey
A
Sent: Tuesday, July 10, 2007 7:23 AM
To: [log in to unmask]
Subject: [TN] Injury by array

Oh wise and wonderful members of tech net -

We have had to incidents in the past six months where assemblers have
been cut while handling assembly arrays (2-up panels) for one of our
products. This has elevated the issue to "Panic Mode" due to the
involvement of EHS&Q (environmental health, safety and quality). As the
designer of the array I have been given ownership of the issue and am
task with resolving it.  After 20+years of handling boards and arrays I
have never been cut, so I am unsure as to what if any corrective action
can be taken to prevent future injuries.

The specifics on the arrays -
10.5" [267mm] x 12.0" [305mm] x 0.062" [1.6mm] thick
2 - up for 4.7"[119.3mm] x 9.2" [233.6mm] PCB
Minimum rail 0.38"[9.5mm]
Tab Route and Retain (mouse bite)
Injuries occurred during loading of the solder printer and during slide
line operations for post reflow assembly.

Any suggestions on what to tell our production group?

Jeffrey McGlaughlin, CID
Engineering Designer
Battelle
505 King Avenue
Columbus Ohio 43201-2693
(614)424-7582 Phone
(614)458-7582 Fax
PS Don't you just love all those  management buzzwords (underlined.)
>;-D

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------



---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------



CONFIDENTIALITY NOTICE: 
This e-mail, and any attachments, is for the sole use of the intended 
recipient(s) and may contain information that is confidential and 
protected from disclosure under the law. Any unauthorized review, use, 
disclosure, or distribution is prohibited. If you are not the intended 
recipient, please contact the sender by reply e-mail, and delete/destroy 
all copies of the original message and attachments. 
Thank you.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2