Dear Sir,
We have been having a few complaints from our customers regarding problems wrt solderability, especially in SMD and BGA pads with ENIG finish. We have checked the solderability at our end as per IPC and we find it to be acceptable. The customer says he is following the same parameters as that for HASL boards for assembly. Can we get some details on the extra precautions wrt assy of ENIG boards
Rgds
Pradeep.M
AGM - Customer Support
Micropack Limited
Plot#16, Jigani Industrial Area,
Anekal Taluk, Bangalore - 562 106
India
Tel : 91 80 7825223 / 7825224
-------------------------------
Micropack Ltd, Bangalore, India
!-- Virus-Free Mail Using AntiVirus for IQ Mail & QuickHeal Engine --!
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|