Having manufactured both hi-tech cleaning machines and sophisticated
ionic contamination testers in the past, I concur with what Steve Pence
stated. I held a patent (now in the public domain) for what was
essentially the opposite: an ionic contamination tester that doubled as
a cleaning machine (I never put it into production as lab tests proved
that it was inefficient as a cleaner). In reality, cleaning machines
with recirculation through DI and carbon columns were never brilliant as
not all contaminants were removed, depending on the spectrum of
adsorption of the carbon, which could not cover all the molecules coming
off the boards. For this reason, all our machines had an open circuit
final rinse with fresh carbon-filtered DI water. In fact, we stopped
making recirculatory rinse machines in 1978, even though the final rinse
was open circuit. All our later machines, until we stopped making them
in 1997, were 100% open circuit DI rinse, using a unique economical system.
Brian
- bogert wrote:
> July 26, 2007
>
> I have a question to pose for Tech Net folks based on my limited
> experience in this area. If I have a cleaning machine that includes a
> built in continuous test for rinse water or wash water resistivity, do I
> need to then still do an independent ionic contamination test using the
> standard DI Water/Alcohol Ionic Contamination test? If so why? What is
> the technical relationship between the two tests? Can one equate the
> cleaning machine Resistivity Test results to the J-STD-001 cleanliness
> limits or the results of the Ionic Contamination test? If so, how?
> Have folks experience shown that one can pass the cleaning machine
> Resistivity Test and still fail Ionic Contamination Test? Why?
>
> Doug, Pauls, as the worlds (wow) expert in this area, what do you say
> (It depends)???.
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
> ext.2815
> -----------------------------------------------------
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|