TECHNET Archives

July 2007

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Wed, 25 Jul 2007 09:35:59 EDT
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="UTF-8"
From:
Werner Engelmaier <[log in to unmask]>
Parts/Attachments:
text/plain (34 lines)
Hi Gebhard,
Thanks for the reference—it would have been clear to me if you had mentioned 
the White Paper I co-authored with Laura Turbini.
You are reading things into what I wrote that I did not say. I wrote: 
"Require a nominal copper deposit thickness of 1.2 mils (30 micro-m) to 
obtain actual plating thicknesses in the range of 1.0 to 1.5 mils (25 to 38 
micro-m);"
I also state that: "A plating thickness of ~25 micro-m (~1.0 mils) has been 
found the minimum thickness to give good reliability; a plating thickness of 
~38 micro-m (~1.5 mils) is optimum from a reliability perspective. Plating 
thicknesses greater than that tends to promote shoulder fractures."
So, I did not say that 38 micro-m (1.5 mils) should be the maximum plating 
thickness.



Werner



**************************************
 Get a sneak peek of the all-new AOL at 
http://discover.aol.com/memed/aolcom30tour

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2