I believe you are correct and a solution is to use dissipative corrugated.
You may not be correct that the cardboard and wood would measure in the
insulative range, but that would only be due to them being hygroscopic and
they would measure high when environment became dryer. It is not an
acceptable ESD protected product. The cardboard is the worksurface which
per ANSI/ESD S20.20-2007 Table 3 has a "required limit" less than 1 x 10E9
ohms.
Per ANSI/ESD S20.20-2007 " ESD damage can occur when:
i. A charged object comes into contact with an ESDS device, or
ii. An ESDS device is grounded while exposed to an electrostatic field."
[ANSI/ESDS20.20 section Foreword] So if the cardboard has a charge, your
product can receive a discharge when the grounded operator handles the
product.
Gene Felder
[log in to unmask]
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of - bogert
Sent: 2007-07-20 6:51 AM
To: [log in to unmask]
Subject: [TN] ESD Question Regarding ANSI/ESD S20.20 and use of cardboard or
wood
July 20, 2007
We have an OEM that has an ESD control program in place per the subject
specification invoked via J-STD-001. However, my position is that he does
not comply with the requirements since during his conformal coating hand
spray process, he places the PWAs ontop of cardboard then sprays them with
coating (no ionizer machine is used in the coating area). Additionally,
sometimes ESD sensitive assemblies are placed on top of cardboard or wooden
blocks during the assembly or inspection process. In all cases when wood or
cardboard is used, the wood and cardboard rests ontop of a properly grounded
ESD mat, and the operator is grounded via a properly connected wrist strap.
I maintain that this practice violates the subject specification since wood
and cardboard are insulating materials which are not to be used at the
workstations, and if one took a surface insulation resistance measurement
across the wood or cardboard surface, one would obviously not meet the value
specified for a properly grounded mat.
I would appreciate any comment on the above, and whether other folks use
wood or cardboard upon which ESD assemblies rest. How do other folks
support assemblies during conformal coating or assembly/inspection if wood
or cardboard is not used?
If the operator is properly grounded via a wrist strap, would any static
charge that may exist on the cardboard or wood surface dissipate through the
wrist strap without damage to the product? I suspect not otherwise there
would be no need to require that the grounded mats be used.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|