Rich,
As someone has said before me, "it all depends" ...
I have known places making industrial types of wire bonded products that were 'maybe' as good as Class 100K [<100,000 particles of 0.5µm size, per cubic foot, and <700 particles of 5µm size, per cubic foot]
I'll stick my neck out and say that it is likely that most facilities employing fine wire bonding [<2 mil ~80µm] are in the Class 1K to 10K range. Something as 'macro' as heavy wire aluminum is totally different.
It depends on what you make - Space level with PIND requirements? Optical application? Jelly-bean commercial parts?
We are either Class 1,000 or 10,000 - depending on the product and the clean room.
Hope that helps
Steve
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Richard Kraszewski
Sent: Friday, July 20, 2007 9:41 AM
To: [log in to unmask]
Subject: [TN] Wire bonding Clean Rooms?
Could anyone share with me the level (if any) of cleanroom you maintain
for your wire bonding operations?
Are you aware of any industry standards that would cover this topic?
Thanks
Rich K
THE INFORMATION CONTAINED IN THIS E-MAIL MESSAGE AND ANY ATTACHMENTS SENT FROM GENTEX CORPORATION IS GENTEX CONFIDENTIAL INFORMATION INTENDED ONLY FOR THE PERSONAL USE OF THE INDIVIDUAL OR ENTITY NAMED ABOVE. If you are not the intended recipient, you are hereby notified that any review, distribution, or copying of this communication is strictly prohibited. If you have received this communication in error, please immediately notify the sender by return e-mail, and delete this e-mail message and any attachments from your computer.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|