Subject: | |
From: | |
Reply To: | |
Date: | Fri, 8 Jun 2007 14:23:40 -0400 |
Content-Type: | text/plain |
Parts/Attachments: |
|
|
You can use an island stencil which can be used to isolate components that you specify. These island stencils will add more volume of paste to the pre-defined area rather than to the whole board. Who do you order your stencils from?
Ronald D. Peeler Jr., B.S. IE
Process Engineer
SWEMCO
Moorestown, NJ 08057
Tel: (856).222.9900 ext. 31
Cel: (484).948.0779
Fax: (856).222.0700
[log in to unmask]
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Gregg A. Owens
Sent: Friday, June 08, 2007 2:06 PM
To: [log in to unmask]
Subject: [TN] Solder Stencil - Insufficient Solder
Dear TechNetters:
Continuing with the theme of insufficient solder. Have a student with a similar problem. They have a few SMT components that are very large (in relation to the majority of others on the PCB). These larger components then have insufficient solder necessitating too much touchup/rework to be cost effective. Is there a way to increase the quantity of solder paste being applied to these specific components using a stencil other than increasing the aperture? Any other ideas?
Thanks,
Gregg Owens, MIT
Manufacturing Technology Training Center, Inc.
Mira Loma, CA 91752
Gregg
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|