Thanks to all that have responded. I also am a firm believer in Heller.
However, there are some particular situations where a standard Heller or
Conceptronics workhorse may not be the best choice.
I know a number of you out there are using BTU Pyramax and Electrovert
OmniFlex reflow ovens. Anyone care to comment on how well they like
those two particular types of ovens utilizing Computational Fluid
Dynamics and jet impingment technology?
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Kevin Glidden
Sent: Wednesday, June 06, 2007 11:40 AM
To: [log in to unmask]
Subject: Re: [TN] Reflow ovens
Ditto. I had Heller succesfully profile a 29"x29"x0.400" PCB that
weighed almost 35 lbs to a traditional ramp-soak-spike profile with no
problems.
I just purchased a Heller last week :)
Kevin Glidden
Manufacturing Engineer
Luminescent Systems Inc.
-----Original Message-----
From: Dehoyos, Ramon [mailto:[log in to unmask]]
Sent: Wednesday, June 06, 2007 12:24 PM
To: [log in to unmask]
Subject: Re: [TN] Reflow ovens
Heller
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard D.
Sent: Tuesday, June 05, 2007 5:57 PM
To: [log in to unmask]
Subject: [TN] Reflow ovens
Anybody out there using the new Scienscope nitrogen reflow ovens? I was
not
even aware Sciencscope made a reflow oven, and was wondering if anybody
has
any hands-on experience with them? Send me your response by direct email
if
you prefer. I would appreciate all feedback, even reports from others
you
may have heard.
And a short poll: if you were going to purchase a new reflow oven today,
what would it be? You will be assembling military, telecommunications,
and
industrial products, both 63/37 and lead-free, and conventional size
pwbs
but some heavy backplanes as well.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit
IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|