You might think you are joking about changing the battery in an
IPOD............
About 2 months ago I was stood at the counter in Kragens waiting to be
served. The guy in front of me is asking the mechanic "do you sell batteries
here for electric vehicles" - mechanic looks blank and answers no - guy
walks off........I had visions of him swapping out the batteries in his
Prius in the parking lot...
John
John Burke
(408) 515 4992
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Guy Ramsey
Sent: Monday, June 18, 2007 10:28 AM
To: [log in to unmask]
Subject: Re: [TN] Failure statistics breakdown data?
Are you talking field return or OEM in factory initial turn on.
If you are talking in-factory initial turn-on, typical device, solder
defects number 1. Mostly opens because shorts are easy to detect with
inspection and ICT. Though in my experience there special events on the
factory floor that can change all that.
If you are talking field returns, we have another story. And must include,
electronic design problems, mechanical design problems and customer abuse or
misuse.
I kept this kind of data at an Organ Company for years. The data set ran
from 1986 to 2000. We stored the information on a VAX 8300. I left in May of
2000. I doubt they continued to collect and analyze the data as that machine
was expensive to maintain and in a DataTrieve database, not easy to port
over to Windows.
I can tell you this. During that time there were periods when field failures
were primarily design related, others when failures were primarily board
fab. related, periods when failures were primarily component related
(sometimes semi-conductor other times passives) and other periods where
failures were primarily related to manufacturing problems. All of these
would be embarrassing for some interested party because they were
attributable to some special cause of failure and we were able to identify
that special cause.
There were very few periods in which the population of defects would not
have been influenced by one of these assignable causes. So, even this huge
data set would not tell you want the most common "common cause" defect would
be. My gut tells me it would be customer misuse followed by, in the case of
Allen Organ, electrical or mechanical design problem.
Other companies might have more design problems than misuse problems. BTW
these merge. You can have a design problem that customers attempt to fix,
which turns into a misuse problem . . . . Ever tried to change a battery in
an iPod? Is an unsuccessful attempt a design problem or customer misuse?
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Joe Fjelstad
Sent: Monday, June 18, 2007 10:59 AM
To: [log in to unmask]
Subject: [TN] Failure statistics breakdown data?
Good (time of day here) colleagues,
Does anyone know of a statistical base that identifies assembly failures
and traces them to causes with some sort of breakdown?
That is failures traced to assembly only (e.g., opens, shorts, insufficient
cleaning, etc.), failures related to PCB manufacturing only (e.g., PTH
failure, opens, shorts, CAF, etc.) and failures traced to the components
themselves of any cause (ESD, overheating, thermal cycling failure, etc.).
I realize that this may be a sensitive topic for some folks and am thus
open to taking any such data off line.
However any perspective based on experience and "guessimates" from the
general audience is encouraged and most welcomed to see if there is any kind
of consensus of experience and how close it matches with the the industry's
general perceptions.
Rough (in the same city at the ball park) estimates are OK.
Thanks in advance for any form of light that can be shed while I fumble
around in the dark feeling for the "main lightswitch". ;-)
Best to all,
Joe
************************************** See what's free at
http://www.aol.com.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|