OKEE, Ioan, offline.
Obviously lots of German-speaking on TN.
Als Christoph Columbus seinerzeit Amerika entdeckte, hatte er natürlich
auch Schwaben an Bord seines Schiffes. Nachdem die Mannschaft an Land
gegangen war, schrie also ein Matrose in die Menge: "Isch au oiner von
Böblinga drbei?" Da erscholl es mitten aus den "First People": "Noi,
abr aus Sendlfenga!".
Sindelfingen is known for the Daimler plant and Böblingen for glass and
IBM. IBM had the most advanced thickfilm MCM plant in the world, fully
automated production of modules for super computers. Don't know if it
exists still.
Inge
-----Ursprungligt meddelande-----
Från: TechNet [mailto:[log in to unmask]] För Tempea, Ioan
Skickat: den 14 juni 2007 19:15
Till: [log in to unmask]
Ämne: Re: [TN] SV: [TN] Nickel barrier and RF applications
I just did, believe me. I did practice a lot, long time ago, in my
German classes. Easy words like
LandwirtschafltlicheProdukzionGenossenschaft are always a good start...
Can I have my file now ;o)
Regards,
Ioan
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Hfjord
Sent: Thursday, June 14, 2007 12:27 PM
To: [log in to unmask]
Subject: [TN] SV: [TN] Nickel barrier and RF applications
On one condition, Ioan. You must say following failure free and with no
pause or hesitation, repeated 5 times in 15 seconds:
"What wood would a woodpeck peck if a woodpeck could peck wood"
Someone got to check you on Friday
Inge
-----Ursprungligt meddelande-----
Från: TechNet [mailto:[log in to unmask]] För Tempea, Ioan
Skickat: den 14 juni 2007 17:34
Till: [log in to unmask]
Ämne: Re: [TN] Nickel barrier and RF applications
Inge,
OK, I'll ask the question: is this report available somewhere? Would
you...
Thanks,
Ioan
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Hernefjord Ingemar
Sent: Thursday, June 14, 2007 4:19 AM
To: [log in to unmask]
Subject: Re: [TN] Nickel barrier and RF applications
Now, Paymon's case was not a RF unit, but sort of a magnetic one, but as
many are interested in microwave issues I noted some matters years ago,
one connected to flux, the other to barrier layers. Sandia Labs had
something called 'Low Residue Soldering Task Force'. Dr Laura Turbini
and her group found a clear connection between the solder residues and
increased RF loss.
>From her report: 'It has been shown that polyglycols and hydrobromic
acid (constituents in some fluxes)diffuses into epoxy during the HASL
process. Under the humid conditions of this test, these processing
chemicals may change the dielectric properties of the test board, which
affect the RF signal integrity.' 451
After that report and some others, we are more motivated to keep
critical RF boards as clean as possible. Normally, flux residues are not
an issue, but some regions of a circuit can be very sensitive to losses.
The other object is rare. I'll send two pictures to Steve's Wax Cabinet.
These show how NiCr leaked out from the edges of the hot RF line and
deposited on the substrate. Caused severe changes in the circuit's RF
properties. We have seen it just a couple of times. No explanation found
how this works. Mystery among many other RF mysteries. The only thing we
could verify was that the 'bleeding' NiCr coincided with the electrical
field.
Inge
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|