Stan,
Get in touch with the guys at www.circuitnettechnology.com they are the masters of board repair material/techniques.
Linda Langley
Jabil Circuit
Training Specialist
(248) 292-6176
CONFIDENTIALITY NOTICE: The information contained in this electronic communication, including any attachments, is confidential information, is intended only for the use of the recipients named above, and may be legally privileged. If the reader of this message is not an intended recipient, you are hereby notified that any review, use, dissemination, distribution or copying of this communication, or any of its contents, is strictly prohibited. If you have received this communication in error, please notify us immediately of the error by return e-mail and please permanently remove the original message and any copy of it from your system. Nothing herein is intended to constitute an electronic signature or consent. Thank you
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Augustin Stan
Sent: Thursday, June 14, 2007 7:47 AM
To: [log in to unmask]
Subject: [TN] Epoxy resins for repairs of Lead Free Assemblies
Hi Technters,
Is anybody which can give an advice regarding a good epoxy resin for repair-
rework assemblies (lifted pads, lands, traces, etc)? What I tried until now, CTC
and Bondmaster, it suffers a lot of softening at lead free temperatures
despite all manufactures recommendations for curing?
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|