Ron, we are still talking about something we don't see. An image or two
would be nice. Yesterday, we opened a big box filled with fresh J
standards you all refer to. Very impressive books indeed. What a lot of
work behind! However, soldering and solder joints can't always be fully
diagnosed with book in hand. My granma had a special way for judging if
the bread in the oven was ready or not. She too them out with a cloth,
knocked on the piece and listened! So am I. While the others are
debating, I use to steal a board and have a look in my lab. And try to
let experience talk. Fortunately, I have not seen the ideal solder joint
yet, and I think I don't want see it either. In fact, not many boards
have been failure reported among the many millions we have made, many
with far from perfect solder joints (according to the standards).
Inge
-----Ursprungligt meddelande-----
Från: TechNet [mailto:[log in to unmask]] För Ron Peeler
Skickat: den 11 juni 2007 19:49
Till: [log in to unmask]
Ämne: Re: [TN] Insufficient Solder
I was referring to SMT, but thanks for the input. Looking @ my process
again is my first step in all this. If I am getting good prints and the
SMT ops are pushing boards through then at least I know that is covered.
However when it comes to dealing with the people in the cells, well that
is a whole different monster.
Ronald D. Peeler Jr., B.S. IE
Process Engineer
SWEMCO
Moorestown, NJ 08057
Tel: (856).222.9900 ext. 31
Cel: (484).948.0779
Fax: (856).222.0700
[log in to unmask]
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Bev Christian
Sent: Monday, June 11, 2007 1:43 PM
To: [log in to unmask]
Subject: Re: [TN] Insufficient Solder
Ron,
Short answer: no.
The problem is there is no one cause. If you do a fishbone diagram (man,
machine, materials and method) you will end up with a pretty big fish
for insufficients. And I didn't even see the original e-mail, so I am
not sure if you are talking about PTH or SMT!
So, obviously, your main thing is to have your process in "control". I
use quotation marks because it depends on what your level of tolerance
for errors is.
The second and less productive possibility is inspection. I would avoid
this as much as possible.
I know my reply deals more with philosophy than specifics, but I thought
it was worth saying.
Regards,
Bev
RIM
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Glen Herzog
Sent: Monday, June 11, 2007 1:12 PM
To: [log in to unmask]
Subject: Re: [TN] Insufficient Solder
Ron,
Your question, "Does anyone here have a sure fire way to combat
insufficient
solder." apparently has two interpretations (1) how do I get sufficient
solder
and (2) What should my inspectors do when there is insufficient solder.
I'll try
to address the inspector issue.
Normally, inspectors do not cause rework. They have criteria from
J-STD-001
and ANSI/IPC-A-610. Based on that criteria they will determine if an
assembly
passes or fails the criteria. Unless that Inspector is quite
experienced, a
Quality Technician or Engineer, or a Process Engineer determines what
action
must be taken. Often "Insufficient Solder' is a process indicator. The
process
needs improved, but the board does not need to be reworked.
Incidentally, I don't think that the term "Insufficient Solder" is in
either
standard. I think that it is just a general term that we often use
without
much definition.
Good Luck, Ron
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential
information, privileged material (including material protected by the
solicitor-client or other applicable privileges), or constitute
non-public information. Any use of this information by anyone other than
the intended recipient is prohibited. If you have received this
transmission in error, please immediately reply to the sender and delete
this information from your system. Use, dissemination, distribution, or
reproduction of this transmission by unintended recipients is not
authorized and may be unlawful.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|