TECHNET Archives

June 2007

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, arnaud grivon <[log in to unmask]>
Date:
Mon, 11 Jun 2007 10:04:36 +0200
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Hernefjord Ingemar <[log in to unmask]>
Subject:
From:
Hernefjord Ingemar <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (99 lines)
Equal heat distribution, dear Arnoud.
Inge 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of arnaud grivon
Sent: den 11 juni 2007 09:43
To: [log in to unmask]
Subject: Re: [TN] SV: [TN] SV: [TN] Z-axis expansion

Hello,

I did not exactly catch your statement of "securing BGA soldering with a vapour phase". Could you expand on that?
Are you saying that your solution consists in reworking BGAs first and then vapour solder the whole reworked assembly?
I thank you in advance for your insight.
Best regards,

Arnaud Grivon
Hfjord a écrit :
> Agree, we bought a vapour phase inline machine in order to secure the 
> BGA soldering.
> Inge
>
> -----Ursprungligt meddelande-----
> Från: TechNet [mailto:[log in to unmask]] För Werner Engelmaier
> Skickat: den 9 juni 2007 02:07
> Till: [log in to unmask]
> Ämne: Re: [TN] SV: [TN] Z-axis expansion
>
> Hi Dave,
> This amount of rework, particularly at LF-temperatures, is not a good 
> idea as you surmised. That can consume upwards of 30% of the fatigue 
> life of the
>
> vias, provided they survive the procedure.
> If you indeed to 'cold' solder joints-this would mean SJs near the BGA 
> centers, you need to 'up' the soldering profile. Reworking these is 
> quite hard to do, bnecause it is difficult to get sufficient heat 
> under the BGAs-that is the reason why vapor phase soldering is making 
> a come-back.
>
> Werner
>
>
>
> **************************************
>  See what's free at http://www.aol.com.
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0 To 
> unsubscribe, send a message to [log in to unmask] with following text in 
> the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt 
> or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing 
> per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
> http://listserv.ipc.org/archives
> Please visit IPC web site
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional 
> information, or contact Keach Sasamori at [log in to unmask] or 
> 847-615-7100
> ext.2815
> -----------------------------------------------------
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0 To 
> unsubscribe, send a message to [log in to unmask] with following text in 
> the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt 
> or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET 
> Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the 
> posts: send e-mail to [log in to unmask]: SET Technet Digest Search the 
> archives of previous posts at: http://listserv.ipc.org/archives Please 
> visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
> for additional information, or contact Keach Sasamori at 
> [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
>   

-- 

----------------------------------------------------------------------

"The information contained in this e-mail/fax and any attachments are the property of THALES and may be confidential. If you are not the intended recipient, please notify us immediately, send this message back to us and destroy it. You are hereby notified that any review, dissemination, distribution, copying or otherwise use of this e-mail/fax is strictly prohibited." 


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2