Very correct Inge -- As always!
Ian
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Hfjord
Sent: Friday, June 22, 2007 4:49 PM
To: [log in to unmask]
Subject: [TN] SV: [TN] Gold finger pitting
Hydrogen?
Inge
-----Ursprungligt meddelande-----
Från: TechNet [mailto:[log in to unmask]] För Genny Gibbard
Skickat: den 22 juni 2007 22:27
Till: [log in to unmask]
Ämne: Re: [TN] Gold finger pitting
Yes, Ian was probably right when he said it was in the nickel, not the
copper. Pardon me for the confusion.
Any other info on the potential problems that could result?
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ido Mashall
Sent: June 22, 2007 2:15 PM
To: [log in to unmask]
Subject: Re: [TN] Gold finger pitting
Didn't they plate nickel before the gold??
I do not see pitting in the copper outside the gold plated area
Ido Mashall
Beyond Materials Ltd.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Genny Gibbard
Sent: Friday, June 22, 2007 10:53 PM
To: [log in to unmask]
Subject: [TN] Gold finger pitting
Please see the picture. We believe the copper underneath the gold is
where the pitting occurs. It appears fully plated with gold, even in
the pits.
It doesn't seem to meet the IPC-600 spec, but I was wondering what are
the potential problems this could cause.
________________________________
From: Steve Gregory [mailto:[log in to unmask]]
Sent: June 22, 2007 1:49 PM
To: Genny Gibbard
Subject: RE: Gold finger pitting
Hi Genny!
It's up! Go to:
http://stevezeva.homestead.com/files/Pitted_Gold_Fingers.jpg
I don't know if I would accept it either. Is it the gold that's pitted,
or the copper beneath it? Or can you tell?
Have a good weekend!
Steve
________________________________
From: Genny Gibbard [mailto:[log in to unmask]]
Sent: Friday, June 22, 2007 1:45 PM
To: Steve Gregory
Subject: Gold finger pitting
Steve could you please help me out here and post a pic?
I need the learned response of Technetters.
This does not appear to meet IPC, but I am not sure what the hazards of
letting it go thru would be.
<<pitted gold fingers.pdf>>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or
847-615-7100 ext.2815
-----------------------------------------------------
--
No virus found in this incoming message.
Checked by AVG Free Edition.
Version: 7.5.472 / Virus Database: 269.9.4/860 - Release Date:
21/06/2007
17:53
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|